Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

AK Steel Aluminized Carbon Steel, Extra Deep Drawing Steel Plus (EDDS+), Standard Grade

Category Metal , Ferrous Metal , Carbon Steel , Low Carbon Steel
Manufacturer AK Steel
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF AK Steel Aluminized Carbon Steel, Extra Deep Drawing Steel Plus (EDDS+), Standard Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Aluminized Type 1 coating contains approximately 91% aluminum and 9% silicon that is metallurgically bonded to the low-carbon steel substrate. Interstitial Free (I-F) steels are made by adding titanium and/or columbium to the molten steel after vacuum degassing and offer excellent drawability.Information provided by AK Steel
Physical Properties Metric English Comments
Density 7.85 g/cc
0.284 lb/in³
Typical Carbon Steel
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 310 MPa
45000 psi
Tensile Strength, Yield 165 MPa
23900 psi
Elongation at Break 44 %
44 %
Modulus of Elasticity 201 GPa
29200 ksi
88.3 GPa

@Temperature 649 °C
12800 ksi

@Temperature 1200 °F
183 GPa

@Temperature 316 °C
26500 ksi

@Temperature 600 °F
Thermal Properties Metric English Comments
Maximum Service Temperature, Air >= 677 °C
>= 1250 °F
Descriptive Properties Value Comments
Deep-Drawing Capability rm 1.8
Strain Hardening Exponent n 0.22