Material Notes:
Description: An advanced ceramic composite formulated to protect equipment from aggressive chemical attack, corrosion, and erosion. The product is a low viscosity composite that is easily applied by brush or roller. ARC 855 may be applied at a minimum thickness of 250 microns (10 mills) per coat. Non-shrinking. 100% Solids. ARC 855 may be used alone, or in conjunction with other ARC composites. This two-coat system provides extended wear and predictable preventative maintenance. The cured ceramic composite provides outstanding chemical and abrasion resistance with a high gloss finish.Benefits:High gloss surface reduces dray, improves flow and pump efficiencyTough resin structure resists thermal-mechanical shockOutstanding adhesion insures reliable performance with no undercutting or under film corrosionLabor and downtime costs are reduced due to ease of applicationNo heat curing requiredPerforms well under fluctuating chemical environments Suggested Uses:Fans & HousingsHeat ExchangersHoppersHydropulpersPump CasingsSand Filter VesselsStructural SteelTanks and VesselsVolutesWet ScrubbersValvesCoal Hoppers and FeedersWaterboxesCooling Water PumpsWear PlatesCoal ScreensImpellersCondensersVacuum PumpsPitted Tanks and PipesPulp Dewatering ScrewsInformation provided by Chesterton
Physical Properties Metric English Comments
Density 1.60 g/cc
0.0578 lb/in³
Cured
Mechanical Properties Metric English Comments
Hardness, Rockwell R 105
105
ASTM D785
Hardness, Shore D 85
85
ASTM D2240
Tensile Strength at Break 23.4 MPa
3400 psi
ASTM D638
Flexural Strength 55.2 MPa
8000 psi
ASTM D790
Compressive Strength 82.7 MPa
12000 psi
ASTM D695
Thermal Properties Metric English Comments
CTE, linear 46.8 µm/m-°C
26.0 µin/in-°F
ASTM C531
Maximum Service Temperature, Air 12.0 °C
53.6 °F
Dry Service
65.0 °C
149 °F
Wet Service
Processing Properties Metric English Comments
Cure Time 120 min

@Temperature 32.0 °C
2.00 hour

@Temperature 89.6 °F
Tack Free
240 min

@Temperature 25.0 °C
4.00 hour

@Temperature 77.0 °F
Tack Free
360 min

@Temperature 32.0 °C
6.00 hour

@Temperature 89.6 °F
Light Load
480 min

@Temperature 16.0 °C
8.00 hour

@Temperature 60.8 °F
Tack Free
600 min

@Temperature 32.0 °C
10.0 hour

@Temperature 89.6 °F
Overend Coat
720 min

@Temperature 25.0 °C
12.0 hour

@Temperature 77.0 °F
Light Load
720 min

@Temperature 32.0 °C
12.0 hour

@Temperature 89.6 °F
Full Load
960 min

@Temperature 10.0 °C
16.0 hour

@Temperature 50.0 °F
Tack Free
1200 min

@Temperature 25.0 °C
20.0 hour

@Temperature 77.0 °F
Overend Coat
1440 min

@Temperature 16.0 °C
24.0 hour

@Temperature 60.8 °F
Light Load
1440 min

@Temperature 25.0 °C
24.0 hour

@Temperature 77.0 °F
Full Load
1440 min

@Temperature 32.0 °C
24.0 hour

@Temperature 89.6 °F
Full Chemical
1920 min

@Temperature 16.0 °C
32.0 hour

@Temperature 60.8 °F
Overend Coat
2160 min

@Temperature 10.0 °C
36.0 hour

@Temperature 50.0 °F
Light Load
2520 min

@Temperature 10.0 °C
42.0 hour

@Temperature 50.0 °F
Overend Coat
2880 min

@Temperature 16.0 °C
48.0 hour

@Temperature 60.8 °F
Full Load
2880 min

@Temperature 25.0 °C
48.0 hour

@Temperature 77.0 °F
Full Chemical
5760 min

@Temperature 10.0 °C
96.0 hour

@Temperature 50.0 °F
Full Load
5760 min

@Temperature 16.0 °C
96.0 hour

@Temperature 60.8 °F
Full Chemical
7680 min

@Temperature 10.0 °C
128 hour

@Temperature 50.0 °F
Full Chemical
Descriptive Properties Value Comments
Color Black
Gray