Atom Adhesives AA-DUCT N02 Epoxy Adhesive

Category Polymer , Thermoset , Epoxy , Epoxy Adhesive
Manufacturer Atom Adhesives
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Atom Adhesives AA-DUCT N02 Epoxy Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AA-DUCT N02 is a single component, heat curing, conductive epoxy polymer that was designed for ease in handling. This high performance conductive polymer cures quickly at elevated temperatures making it ideally suited for rapid Processing and assembly. AA-DUCT N02 passes NASA’s outgassing testing (ASTM E-595) and is listed in NASA’s Outgassing Data for Selecting Spacecraft Materials list. AA-DUCT N02 offers excellent mechanical, electrical, and physical properties at continuous operating Temperatures up To 175°C. This versatile silver conductive adhesive can be used for chip bonding in Micro and electronic hybrid circuit Fabrication. This unique conductive polymer also exhibits outstanding adhesion to a wide variety of substrates with good hot strength at intermittent temperatures up to 325°C. AA-DUCT N02 has also been used in microwave applications for EMI and FRI shielding, for assembly and repair of circuit boards and Electronic component manufacturing.Appearance: GreyCure Type: Heat cure or Room temperatureMix Ratio by weight: 100:6/Resin:HardenerBenefits: High strengthPerfect bondCold solder for heat sensitive componentsWave guides Substrates: Excellent choice for Integrated Circuits, aluminum, copper, magnesium, steel, bronze, nickel, kovar, ceramic, glass, phenolic and G-10 epoxy glass boards. Typical Application: Microwave applications for EMI and FRI shielding, for assembly and repair of circuit boards and Electronic component manufacturing.Information provided by Atom Adhesives
Physical Properties Metric English Comments
Outgassing - Total Mass Loss 0.00 %
0.00 %
CVCM
0.070 %
0.070 %
WVR
0.25 %
0.25 %
TTML
Mechanical Properties Metric English Comments
Hardness, Shore D 88
88
cured
Thermal Properties Metric English Comments
Thermal Conductivity 1.46 W/m-K
10.1 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 175 °C
347 °F
Minimum Service Temperature, Air -55.0 °C
-67.0 °F
Electrical Properties Metric English Comments
Volume Resistivity 0.038 ohm-cm
0.038 ohm-cm
cured
Processing Properties Metric English Comments
Cure Time 30.0 min

@Temperature 175 °C
0.500 hour

@Temperature 347 °F
60.0 min

@Temperature 150 °C
1.00 hour

@Temperature 302 °F
120 min

@Temperature 125 °C
2.00 hour

@Temperature 257 °F
Shelf Life 6.00 Month
6.00 Month
Descriptive Properties Value Comments
Viscosity Soft paste