Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 2400 °C | 4350 °F | |
MarkeTech Zirconium Oxide Ceramic - Zirconia, Y2O3 Stabilized Data provided by the supplier, MarkeTech International.Zirconium oxide is widely used and has superior high temperature properties. When combined with yttria the strength and fracture toughness is .. |
|||
Maximum Service Temperature, Air | 2400 °C | 4350 °F | |
ICE ZrO Data provided by the manufacturer, International Ceramic Engineering. |
|||
Maximum Service Temperature, Air | 2400 °C | 4350 °F | |
Zircar Zirconia ZOG Single Crystal Zirconia Grog Insulation Zircar Zirconia Single Crystal Grog Type ZOG is composed of small (0.6 to 2.4mm) single crystals of zirconia having a monoclinic structure. These "skull melted" crystallites exhibit virtually no par.. |
|||
Maximum Service Temperature, Air | 2400 °C | 4350 °F | NO-LOAD COND. |
CoorsTek ZDY Yttria Fully Stabilized Zirconia Oxygen ionic conductor for high-stress and high-thermal-shock environments |
|||
Maximum Service Temperature, Air | 2400 °C | 4350 °F | |
Anderman Ceramics EZY 94 Zirconia, 94%, Yttria-Stabilized Dense impervious zirconia for high wear and aggressive engineering applications. Available in many shapes and sizes.Information provided by Anderman Ceramics. |
|||
Maximum Service Temperature, Air | 2400 °C | 4350 °F | no load |
Astro Met AmZirOx 86 Zirconia - Zirconium Oxide General Description:AmZirOx 86 zirconia (Astro Met Zirconium Oxide) is a yttria stabilized zirconia ceramic material which features high strength and toughness making it a candidate material for use.. |
|||
Maximum Service Temperature, Air | 2400 °C | 4350 °F | |
Zircar Zirconia ZOG Single Crystal Zirconia Grog Insulation Zircar Zirconia Single Crystal Grog Type ZOG is composed of small (0.6 to 2.4mm) single crystals of zirconia having a monoclinic structure. These "skull melted" crystallites exhibit virtually no par.. |
|||
Maximum Service Temperature, Air | 2400 °C | 4350 °F | |
Anderman Ceramics EZC96P Zirconia, 96%, Calcia-Stabilized Available in impervious or porous grades in a range of shapes and sizes.Information provided by Anderman Ceramics. |