Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

CoorsTek ZDY Yttria Fully Stabilized Zirconia

Category Ceramic , Oxide , Zirconium Oxide
Manufacturer CoorsTek
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CoorsTek ZDY Yttria Fully Stabilized Zirconia.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Oxygen ionic conductor for high-stress and high-thermal-shock environments
Physical Properties Metric English Comments
Density 5.60 g/cc
0.202 lb/in³
ASTM-C 20
Water Absorption 0.00 %
0.00 %
ASTM-373
Mechanical Properties Metric English Comments
Hardness, Rockwell 45 N 75
75
Modulus of Elasticity 173 GPa
25100 ksi
ASTM-C848
Flexural Strength 207 MPa
30000 psi
MOR; ASTM-F417
Fracture Toughness 3.00 MPa-m½
2.73 ksi-in½
Notched Beam
Thermal Properties Metric English Comments
CTE, linear 10.5 µm/m-°C

@Temperature 25.0 - 1000 °C
5.83 µin/in-°F

@Temperature 77.0 - 1830 °F
ASTM-C372
Thermal Conductivity 2.20 W/m-K
15.3 BTU-in/hr-ft²-°F
ASTM-C408
Maximum Service Temperature, Air 2400 °C
4350 °F
NO-LOAD COND.
Descriptive Properties Value Comments
Color Ivory
Permeability Gas tight
Thermal Shock Resistance (°C) 200
ΔTc
Copyright © lookpolymers.com All Rights Reserved