ICE ZrO

Category Ceramic , Oxide , Zirconium Oxide
Manufacturer International Ceramic Engineering
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ICE ZrO.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the manufacturer, International Ceramic Engineering.
Physical Properties Metric English Comments
Density 6.07 g/cc
0.219 lb/in³
Water Absorption 0.00 %
0.00 %
Mechanical Properties Metric English Comments
Hardness, Mohs 8.7
8.7
Flexural Strength 700 MPa
102000 psi
Fracture Toughness 13.0 MPa-m½
11.8 ksi-in½
Thermal Properties Metric English Comments
CTE, linear 10.3 µm/m-°C

@Temperature 25.0 - 600 °C
5.72 µin/in-°F

@Temperature 77.0 - 1110 °F
Thermal Conductivity 2.20 W/m-K
15.3 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 2400 °C
4350 °F
Descriptive Properties Value Comments
Color Yellow White