Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 70.0 - 135 °C | 158 - 275 °F | Average value: 85.4 °C Grade Count:103 |
Overview of materials for High Density Polyethylene (HDPE), Ultra High Molecular Weight This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Ultra High Molecular Weight". Each property range of values reported i.. |
|||
Maximum Service Temperature, Air | 125 - 135 °C | 257 - 275 °F | Softening Range |
Huntsman Araldite GT 6097 US Bisphenol A Epoxy Solid Resin Weight per Epoxide (EEW, g/eq) 2000 to 2500. Max color is 3.Comments/Applications: Unmodified bis A "Type 7" epoxy. Higher melt viscosity "Type 7" for high quality industrial and thick film powder.. |
|||
Maximum Service Temperature, Air | 120 - 135 °C | 248 - 275 °F | long term; EMS |
EMS-Grivory Grivory® XE 5026 (BG-30 H) PA6-GF30 Product description: Grilon B XE 5026 (BG-30 H) black 9922 is a high heat stabilized, 30% glass fiber reinforced PA6- Injection molding grade with modified flowability. Grilon B XE 5026 (BG-30 H) bl.. |
|||
Maximum Service Temperature, Air | 80.0 - 135 °C | 176 - 275 °F | Average value: 114 °C Grade Count:5 |
Overview of materials for Nylon 6, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, PTFE Filled". Each property range of values reported is minimum and maximum values of appropria.. |