Unifrax Fiberfrax® 970 Ceramic Fiber Paper

Category Ceramic , Oxide , Aluminum Oxide , Silicon Oxide
Manufacturer Unifrax I LLC
Trade Name Fiberfrax®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Unifrax Fiberfrax® 970 Ceramic Fiber Paper.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
970 paper is made from high-purity Fiberfrax washed fiber. During the manufacture of this product, a large portion of the unfiberized particles in the bulk fiber are removed prior to paper lay-up. The washing of the fiber gives great uniformity to the paper's structure while reducing weight and improving the thermal performance; in addition, this product is preferred in automatic die stamping operations where unfiberized particles in the paper can lead to excessive die wear.Information Provided by Unifrax I LLC
Physical Properties Metric English Comments
Density 0.160 g/cc
0.00579 lb/in³
Loss On Ignition 7.0 %
7.0 %
including binder
Mechanical Properties Metric English Comments
Tensile Strength at Break 0.172 MPa
25.0 psi
As manufactured
Tensile Strength, Yield 0.648 MPa
94.0 psi
As manufactured
Compressive Strength 0.00896 MPa
1.30 psi
10% deformation
0.0400 MPa
5.80 psi
25% deformation
0.152 MPa
22.0 psi
50% deformation
Thermal Properties Metric English Comments
Melting Point 1793 °C
3259 °F
Maximum Service Temperature, Air 1100 °C
2010 °F
Recommended Operating Temperature
Component Elements Properties Metric English Comments
Al2O3 47 - 52 %
47 - 52 %
Fe2O3 <= 0.50 %
<= 0.50 %
SiO2 48 - 53 %
48 - 53 %
Descriptive Properties Value Comments
Color White
Fiber Index (% Wt) 70
Na2O3 (%) <0.5
Temperature Grade (°C) 1260