Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

California Fine Wire Stablohm 610 Nickel, Chromium and Iron Resistance Wire

Category Metal , Electronic/Magnetic Alloy , Ferrous Metal
Manufacturer California Fine Wire
Trade Name Stablohm
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF California Fine Wire Stablohm 610 Nickel, Chromium and Iron Resistance Wire.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire.
Physical Properties Metric English Comments
Density 7.94 g/cc
0.287 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength at Break 621 MPa
90000 psi
Annealed
965 MPa
140000 psi
Stress relieved
1210 MPa
175000 psi
Hard
Thermal Properties Metric English Comments
CTE, linear 15.6 µm/m-°C

@Temperature 20.0 °C
8.67 µin/in-°F

@Temperature 68.0 °F
Specific Heat Capacity 0.460 J/g-°C

@Temperature 20.0 °C
0.110 BTU/lb-°F

@Temperature 68.0 °F
Thermal Conductivity 13.0 W/m-K
90.2 BTU-in/hr-ft²-°F
Melting Point 1300 °C
2372 °F
Maximum Service Temperature, Air 980 °C
1800 °F
Operating Temperature
Component Elements Properties Metric English Comments
Chromium, Cr 20 %
20 %
Iron, Fe 45 %
45 %
as balance
Nickel, Ni 35 %
35 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.000101 ohm-cm
0.000101 ohm-cm
3% tolerance on sizes below 0.02, 5% tolerance on sizes above 0.02
Descriptive Properties Value Comments
Magnetic Faint
Temperature Coefficient of Resistance 0.0004 ohms/ohm-°C
0-100°C