Polymer Property : Thermal Conductivity = 57.6 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 8.30 W/m-K
57.6 BTU-in/hr-ft²-°F
TIMET TIMETAL® 15-3 Titanium Alloy (Ti-15V-3Cr-3Sn-3Al), Anneal Strip/Sheet
High-Strength, Cold Formable Strip AlloyIndustry Specifications: USA Aerospace: AMS 4914A.Features: Cold formable and weldable, this strip alloy is primarily used for aircraft ducting, pressure vess..
Thermal Conductivity 8.30 W/m-K
57.6 BTU-in/hr-ft²-°F
TIMET TIMETAL® 15-3 Titanium Alloy (Ti-15V-3Cr-3Sn-3Al); Aged at 482°C
High-Strength, Cold Formable Strip AlloyIndustry Specifications: USA Aerospace: AMS 4914A.Features: Cold formable and weldable, this strip alloy is primarily used for aircraft ducting, pressure vess..
Thermal Conductivity 8.30 W/m-K
57.6 BTU-in/hr-ft²-°F
TIMET TIMETAL® 15-3 Titanium Alloy (Ti-15V-3Cr-3Sn-3Al); Aged at 538°C
High-Strength, Cold Formable Strip AlloyIndustry Specifications: USA Aerospace: AMS 4914A.Features: Cold formable and weldable, this strip alloy is primarily used for aircraft ducting, pressure vess..
Thermal Conductivity 8.30 W/m-K

@Temperature 20.0 - 95.0 °C
57.6 BTU-in/hr-ft²-°F

@Temperature 68.0 - 203 °F
TIMET TIMETAL® 3-2.5 -0.05Pd Titanium Alloy
Cold Workable Medium Strength Alloy. Palladium is added to this grade to enhance its corrosion behavior. Property data below is typical of TIMETAL® 3-2.5 Titanium Alloy.Data provided by TIMET.
Thermal Conductivity 8.30 W/m-K

@Temperature 20.0 - 95.0 °C
57.6 BTU-in/hr-ft²-°F

@Temperature 68.0 - 203 °F
TIMET TIMETAL® 3-2.5 Titanium Alloy (Ti-3Al-2.5V; ASTM Grade 9) Aged
Cold Workable Medium Strength Alloy. UTS, TYS, and elongation data below are specific to aged material; other specific condition entries are also available in MatWeb.Features: Cold formable and we..
Thermal Conductivity 8.30 W/m-K

@Temperature 20.0 - 95.0 °C
57.6 BTU-in/hr-ft²-°F

@Temperature 68.0 - 203 °F
TIMET TIMETAL® 3-2.5 Titanium Alloy (Ti-3Al-2.5V; ASTM Grade 9) Annealed
Cold Workable Medium Strength Alloy. UTS, TYS, Elongation, R.A. and bend radius data below are specific to annealed material; other specific condition entries are also available in MatWeb.Features..
Thermal Conductivity 8.30 W/m-K

@Temperature 20.0 - 95.0 °C
57.6 BTU-in/hr-ft²-°F

@Temperature 68.0 - 203 °F
TIMET TIMETAL® 3-2.5 Titanium Alloy (Ti-3Al-2.5V; ASTM Grade 9) Typical Properties
Cold Workable Medium Strength AlloyFeatures: Cold formable and weldable, this alloy is used primarily for honeycomb foil and hydraulic tubing applications. Industrial applications such as pressure v..
Thermal Conductivity 8.30 W/m-K
57.6 BTU-in/hr-ft²-°F
TIMET TIMETAL® 679 (Ti-11Sn-5Zr-2.25Al-1Mo-0.2Si) Titanium Alloy; Quenched & Aged
High-Temperature, High-Strength Creep Resistant AlloyIndustry Specifications: USA Aerospace: AMS 4974.Features: TIMETAL 679 has excellent tensile strength and is creep resistant up to 450°C. It i..
Thermal Conductivity 8.30 W/m-K

@Temperature 20.0 - 95.0 °C
57.6 BTU-in/hr-ft²-°F

@Temperature 68.0 - 203 °F
TIMET TIMETAL® 3-2.5 Titanium Alloy (Ti-3Al-2.5V; ASTM Grade 9) CWSR
Cold Workable Medium Strength Alloy. UTS, TYS, and elongation data below are specific to CWSR condition; other specific condition entries are also available in MatWeb.Features: Cold formable and w..