Material Notes:
Has nearly the wettability and low temperature malleability of Indium. Solders silver, fired glass, and ceramics. Large plastic range.Information provided by the manufacturer, Indium Corporation.
Physical Properties Metric English Comments
Density 7.54 g/cc
0.272 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 2.7

@Load 100 kg,
Time 30.0 sec
2.7

@Load 220 lb,
Time 0.00833 hour
Tensile Strength, Ultimate 11.4 MPa
1650 psi
Elongation at Break 61 %
61 %
Shear Strength 11.0 MPa
1600 psi
Shear Bond Holding Strength
Thermal Properties Metric English Comments
CTE, linear 15.0 µm/m-°C

@Temperature 20.0 °C
8.33 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 67.0 W/m-K

@Temperature 85.0 °C
465 BTU-in/hr-ft²-°F

@Temperature 185 °F
Melting Point 143 - 237 °C
289 - 459 °F
Solidus 143 °C
289 °F
Liquidus 237 °C
459 °F
Component Elements Properties Metric English Comments
Indium, In 90 %
90 %
Silver, Ag 10 %
10 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000780 ohm-cm
0.00000780 ohm-cm