Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.650 W/m-K | 4.51 BTU-in/hr-ft²-°F | |
Quadrant EPP Borotron® HM PE-HMW + boron based additive (ISO Data) Borotron UH and Borotron HM are boron loaded PE-(U)HMW grades, specifically developed for neutron shielding purposes in nuclear installations. The high hydrogen content of PE-(U)HMW makes it very su.. |
|||
Thermal Conductivity | 0.650 W/m-K | 4.51 BTU-in/hr-ft²-°F | |
Quadrant EPP Borotron® UH PE-UHMW + boron based additive (ISO Data) Borotron UH and Borotron HM are boron loaded PE-(U)HMW grades, specifically developed for neutron shielding purposes in nuclear installations. The high hydrogen content of PE-(U)HMW makes it very su.. |
|||
Thermal Conductivity | 0.650 W/m-K @Temperature 80.0 °C |
4.51 BTU-in/hr-ft²-°F @Temperature 176 °F |
Z Direction; ASTM C518 |
Rogers Corporation RO4450F Prepreg Prepreg is commonly used to inexpensively form less critical signal layers in antenna designs. A high post-cure Tg makes RO4400 series prepreg an excellent choice for multi-layers requiring sequent.. |
|||
Thermal Conductivity | 0.650 W/m-K | 4.51 BTU-in/hr-ft²-°F | |
Aremco Aremco-Bond™ 855 Epoxy Adhesive
(discontinued **) High performance epoxy for specialty bonding and potting applications to 350ºF (175°C). Can be applied to a myriad of substrates, offering exceptional chemical, electrical, and mechanical properti.. |
|||
Thermal Conductivity | 0.650 W/m-K | 4.51 BTU-in/hr-ft²-°F | ASTM C177 |
Solvay Specialty Polymers Torlon® 4275 Polyamide-imide (PAI)
(Unverified Data**) Torlon 4275 is a wear-resistant grade of polyamide-imide (PAI). This grade offers an excellent balance of mechanical properties and wear resistance. It offers high tensile strength and modulus with .. |
|||
Thermal Conductivity | 0.650 W/m-K | 4.51 BTU-in/hr-ft²-°F | |
Chevron Phillips Ryton® R10-110BL Polyphenylene Sulfide Compound
(discontinued **) Black Polyphenylene Sulfide CompoundRyton® R10-110BL is a glass and mineral filled polyphenylene sulfide compound which provides a good combination of mechanical and electrical properties.Applicati.. |
|||
Thermal Conductivity | 0.650 W/m-K | 4.51 BTU-in/hr-ft²-°F | DIN 52612 |
Lehmann & Voss LUVOCOM® 1105-7751 PEEK, with carbon fiber, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
Thermal Conductivity | 0.650 W/m-K | 4.51 BTU-in/hr-ft²-°F | ASTM D177 |
Manifattura Cattaneo RULON® W2 Polytetrafluoroethylene Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
Thermal Conductivity | 0.650 W/m-K | 4.51 BTU-in/hr-ft²-°F | DIN 52612 |
Lehmann & Voss LUVOCOM® 1105-7041 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
Thermal Conductivity | 0.650 W/m-K | 4.51 BTU-in/hr-ft²-°F | |
Schott N-PK51 Glass Suitable for precision moldingInformation Provided by SCHOTT North America, Inc. |
|||
Thermal Conductivity | 0.650 W/m-K | 4.51 BTU-in/hr-ft²-°F | |
Schott SF4 Glass Information Provided by SCHOTT North America, Inc. |
|||
Thermal Conductivity | 0.650 W/m-K | 4.51 BTU-in/hr-ft²-°F | ASTM C177 |
Solvay Specialty Polymers Torlon® 4275 Polyamide-imide (PAI) Torlon® 4275 is a wear-resistant grade of polyamide-imide (PAI). This grade offers an excellent balance of mechanical properties and wear resistance. It offers high tensile strength and modulus w.. |
|||
Thermal Conductivity | 0.650 W/m-K | 4.51 BTU-in/hr-ft²-°F | parallel to thickness |
Zircar Refractory Composites RS-99R Refractory Sheet Type RS-99R boards are prefired and are unaffected by moisture. They stay rigid even if saturated with water.Information provided by ZIRCAR Refractory Composites, Inc. (ZRCI) |
|||
Thermal Conductivity | 0.650 W/m-K | 4.51 BTU-in/hr-ft²-°F | perpendicular to thickness |
Zircar Refractory Composites RS-A Refractory Sheet ZRCI`s Refractory Sheet Type RS-A Moldable is a tough ceramic fiber reinforced insulation which contains no asbestos. Developed as an asbestos board replacement for induction coil liners and molten .. |
|||
Thermal Conductivity | 0.650 W/m-K | 4.51 BTU-in/hr-ft²-°F | parallel to thickness |
Zircar Refractory Composites RS-A1 Refractory Sheet This product is made from Type RS-A Moldable. Type RS-A was developed as an asbestos board replacement for induction coil liners and molten metal transport, and contains no asbestos. Refractory Shee.. |
|||
Thermal Conductivity | 0.650 W/m-K | 4.51 BTU-in/hr-ft²-°F | parallel to thickness |
Zircar Refractory Composites RS-A2 Refractory Sheet This product is made from Type RS-A Moldable. Type RS-A was developed as an asbestos board replacement for induction coil liners and molten metal transport, and contains no asbestos. Refractory Shee.. |
|||
Thermal Conductivity | 0.650 W/m-K | 4.51 BTU-in/hr-ft²-°F | parallel to thickness |
Zircar Refractory Composites RS-A3 Refractory Sheet This product is made from Type RS-A Moldable. Type RS-A was developed as an asbestos board replacement for induction coil liners and molten metal transport, and contains no asbestos. Refractory Shee.. |
|||
Thermal Conductivity | 0.650 W/m-K | 4.51 BTU-in/hr-ft²-°F | ASTM C177 |
Solvay Specialty Polymers Algoflon® 60BZ PTFE; Bronze Filled
(discontinued **) Data provided by the manufacturer.60 wt.% Bronze. Suspension polymer powder grade recommended for compression molding. Pure PTFE possesses high inertness, excellent dielectric properties, almost no .. |
|||
Thermal Conductivity | 0.650 W/m-K | 4.51 BTU-in/hr-ft²-°F | ASTM C177 |
Solvay Specialty Polymers Algoflon® 35CAR B PTFE; Carbon Filled
(discontinued **) Data provided by the manufacturer.35 wt.% Electrog. Carbon Filler. Suspension polymer powder grade recommended for compression molding. Pure PTFE possesses high inertness, excellent dielectric prope.. |