Thermal Conductivity 3.10 W/m-K
21.5 BTU-in/hr-ft²-°F
ASTM E-1461
Ovation Polymers Nemcon™ H PK DP110/X5 PEEK
Thermally Conductive Polyetheretherketone, excellent chemical, high stiffness, modulus and HDT.Information provided by Ovation Polymers
Thermal Conductivity 3.10 W/m-K
21.5 BTU-in/hr-ft²-°F
Internal Method
Ovation Polymers Nemcon™ H PK DP110/X5 Polyetheretherketone
Thermally Conductive Polyetheretherketone, excellent chemical, high stiffness, modulus and HDT. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All sa..
Thermal Conductivity 3.10 W/m-K

@Temperature 20.0 - 400 °C
21.5 BTU-in/hr-ft²-°F

@Temperature 68.0 - 752 °F
China-Yixing Longly Refractories Zirconia Ceramics
LONGLY provides a multitude of zirconia products including balls, plates, tubes, rods and etc. by adopting magnesia, calcia or yttria stabilized zirconia powder as raw material through dry pressing,..
Thermal Conductivity 3.10 W/m-K
21.5 BTU-in/hr-ft²-°F
perpendicular
Carlisle 201LL Carbon-Carbon Composite
Carbon-Carbon Composite manufactured as sheets from 4mm to 125mm thick this material is essentially a fracture tough, fiber reinforced graphite often referred to as a “CFC”. Good for use in air t..