Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 3.10 W/m-K | 21.5 BTU-in/hr-ft²-°F | ASTM E-1461 |
Ovation Polymers Nemcon™ H PK DP110/X5 PEEK Thermally Conductive Polyetheretherketone, excellent chemical, high stiffness, modulus and HDT.Information provided by Ovation Polymers |
|||
Thermal Conductivity | 3.10 W/m-K | 21.5 BTU-in/hr-ft²-°F | Internal Method |
Ovation Polymers Nemcon™ H PK DP110/X5 Polyetheretherketone Thermally Conductive Polyetheretherketone, excellent chemical, high stiffness, modulus and HDT. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All sa.. |
|||
Thermal Conductivity | 3.10 W/m-K @Temperature 20.0 - 400 °C |
21.5 BTU-in/hr-ft²-°F @Temperature 68.0 - 752 °F |
|
China-Yixing Longly Refractories Zirconia Ceramics LONGLY provides a multitude of zirconia products including balls, plates, tubes, rods and etc. by adopting magnesia, calcia or yttria stabilized zirconia powder as raw material through dry pressing,.. |
|||
Thermal Conductivity | 3.10 W/m-K | 21.5 BTU-in/hr-ft²-°F | perpendicular |
Carlisle 201LL Carbon-Carbon Composite Carbon-Carbon Composite manufactured as sheets from 4mm to 125mm thick this material is essentially a fracture tough, fiber reinforced graphite often referred to as a “CFC”. Good for use in air t.. |