Material Notes:
Thermally Conductive Polyetheretherketone, excellent chemical, high stiffness, modulus and HDT. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All samples are prepared according to ASTM standards. Variations within normal tolerances are possible for various types of colors and functional properties like UV resistance.Information provided by Ovation Polymers
Physical Properties Metric English Comments
Specific Gravity 1.52 g/cc
1.52 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Yield 75.0 MPa
10900 psi
50 mm/min; ASTM D638
Elongation at Break 2.5 %
2.5 %
50 mm/min; ASTM D638
Tensile Modulus 6.25 GPa
906 ksi
50 mm/min; ASTM D638
Flexural Yield Strength 135 MPa
19600 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 7.05 GPa
1020 ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 0.325 J/cm
0.609 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Thermal Conductivity 3.10 W/m-K
21.5 BTU-in/hr-ft²-°F
Internal Method
Deflection Temperature at 1.8 MPa (264 psi) 206 °C

@Thickness 3.20 mm
403 °F

@Thickness 0.126 in
unannealed; ASTM D648
Glass Transition Temp, Tg 150 °C
302 °F
ASTM D3482
Electrical Properties Metric English Comments
Surface Resistance 8.00e+12 ohm
8.00e+12 ohm
Internal Method