Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 1.00 - 3.00 W/m-K @Temperature 50.0 - 100 °C |
6.94 - 20.8 BTU-in/hr-ft²-°F @Temperature 122 - 212 °F |
Average value: 1.94 W/m-K Grade Count:14 |
Overview of materials for Silicone, Molded, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Silicone, Molded, Glass Fiber Filled". Each property range of values reported is minimum and maximum val.. |
|||
Thermal Conductivity | 2.00 - 3.00 W/m-K | 13.9 - 20.8 BTU-in/hr-ft²-°F | ASTM C177 |
PolyOne Therma-Tech™ NJ-6000C TC Nylon 12
(discontinued **) Therma-Tech™ Thermal Management Compounds have been engineered to combine the heat transfer and cooling capabilities of metals with the design freedom, weight reduction and cost advantages of therm.. |
|||
Thermal Conductivity | 1.50 - 3.00 W/m-K | 10.4 - 20.8 BTU-in/hr-ft²-°F | in "c" direction |
Momentive Performance Materials Pyrolytic Boron Nitride (PBN) Coating High temperature protective coating for graphite.PBN has become the material of choice for compound semiconductor crystal growth and wafer processing. PBN coatings also seal and protect graphite fr.. |