Momentive Performance Materials Pyrolytic Boron Nitride (PBN) Coating

Category Ceramic , Nitride , Other Engineering Material , Ceramic/Metallic Coating
Manufacturer Momentive Performance Materials (Former GE Advanced Ceramics)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Momentive Performance Materials Pyrolytic Boron Nitride (PBN) Coating.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High temperature protective coating for graphite.PBN has become the material of choice for compound semiconductor crystal growth and wafer processing. PBN coatings also seal and protect graphite from very corrosive atmospheres including most molten metals, all acids, and hot ammonia. PBN is an electrical insulator which exhibits a high degree of anisotropy, e.g. good thermal conductor parallel ("ab") to substrate and thermal insulator through thickness ("c").Information provided by Momentive Performance Materials, formerly GE Advanced Ceramics.
Physical Properties Metric English Comments
Density 1.95 - 2.22 g/cc
0.0704 - 0.0802 lb/in³
Mechanical Properties Metric English Comments
Modulus of Elasticity 22.0 GPa
3190 ksi
Young's modulus
Compressive Strength 220 MPa
31900 psi
Thermal Properties Metric English Comments
CTE, linear 2.00 µm/m-°C

@Temperature 20.0 °C
1.11 µin/in-°F

@Temperature 68.0 °F
ab direction
Thermal Conductivity 1.50 - 3.00 W/m-K
10.4 - 20.8 BTU-in/hr-ft²-°F
in "c" direction
20.0 - 120 W/m-K
139 - 833 BTU-in/hr-ft²-°F
in "ab" direction
Maximum Service Temperature, Air 800 °C
1470 °F
oxidation limit
Decomposition Temperature 2500 °C
4530 °F
Optical Properties Metric English Comments
Emissivity (0-1) 0.50
0.50
normal spectrum
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+9 ohm-cm
1.00e+9 ohm-cm