Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.431 W/m-K | 2.99 BTU-in/hr-ft²-°F | |
Micropol Isoplas P381 Crosslinkable Polyethylene Information provided by Micropol Limited |
|||
Thermal Conductivity | 0.431 W/m-K | 2.99 BTU-in/hr-ft²-°F | |
Micropol Isoplas P471 Crosslinkable Polyethylene Information provided by Micropol Limited |
|||
Thermal Conductivity | 0.431 W/m-K | 2.99 BTU-in/hr-ft²-°F | |
Micropol Isoplas P602 Crosslinkable Polyethylene Information provided by Micropol Limited |