Polymer Property : Thermal Conductivity = 0.431 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.431 W/m-K
2.99 BTU-in/hr-ft²-°F
Micropol Isoplas P381 Crosslinkable Polyethylene
Information provided by Micropol Limited
Thermal Conductivity 0.431 W/m-K
2.99 BTU-in/hr-ft²-°F
Micropol Isoplas P471 Crosslinkable Polyethylene
Information provided by Micropol Limited
Thermal Conductivity 0.431 W/m-K
2.99 BTU-in/hr-ft²-°F
Micropol Isoplas P602 Crosslinkable Polyethylene
Information provided by Micropol Limited