Thermal Properties Metric English Comments
Thermal Conductivity 180 W/m-K
1250 BTU-in/hr-ft²-°F
IBC Advanced Alloys Beralcast® 191 Beryllium-Aluminum Alloy
This alloy consists of 65% Be and 35% Al (by weight) and is used primarily for moderate strength cast electronic and thermal packaging applications. BeAl-191 also provides a unique capability for se..
Thermal Conductivity 180 W/m-K
1250 BTU-in/hr-ft²-°F
Longitudinal
IBC Advanced Alloys Beralcast® 310 Beryllium-Aluminum Alloy
This alloy, a metal matrix composite, consisting of between 60 and 70% Be (by weight) is a wrought product offered by IBC Engineered Materials to be used in the process of manufacturing extrusions f..
Thermal Conductivity 180 - 190 W/m-K
1250 - 1320 BTU-in/hr-ft²-°F
z direction
MarkeTech Cu/Mo/Cu 1:3:1 Laminated Sheet
Cu/MoCu sheets have very high in-plane thermal conductivity provide by layers of Cu and low CTEs provided by the inner layer of molybdenum. These laminated sheets spread heat from a concentrated hea..
Thermal Conductivity 180 - 190 W/m-K
1250 - 1320 BTU-in/hr-ft²-°F
MarkeTech W90Cu Tungsten/Copper Heat Sink Material
WCu composites are made by vacuum infiltration of uniform controlled porous blocks of tungsten with molten copper. This results in a material with an interconnected Cu matrix that has high thermal c..
Thermal Conductivity 180 W/m-K
1250 BTU-in/hr-ft²-°F
Sapco Aluminum Nitride
Information provided by Sapco.
Thermal Conductivity 180 W/m-K
1250 BTU-in/hr-ft²-°F
ASTM E1461
M Cubed Technologies SSC-802 Reaction-Bonded Silicon Carbide
Medium-grained reaction-bonded SiC for high wear applications. Bullnoses, fan liners, hydrocyclone liners, etc. Can be cast into very large shapes (greater than 4 ft. square, 5-6 inches thick)Info..
Thermal Conductivity 180 W/m-K
1250 BTU-in/hr-ft²-°F
DIN EN 821-2 / ASTM-C408
CeramTec Alunit® Aluminum Nitride
Alunit® offers an extremely high thermal conductivity of 180 W/mK and outstanding electrical insulation properties. The thermal expansion coefficient of this material is comparable to silicon. Its ..
Thermal Conductivity 180 W/m-K
1250 BTU-in/hr-ft²-°F
Casting
CMW® 100 Copper Alloy
CMW® 100 material is a heat treatable, high strength, high conductivity copper base alloy. Its properties are a combination of highest strength and hardness with relatively high electrical and ther..
Thermal Conductivity 180 W/m-K
1250 BTU-in/hr-ft²-°F
CMW® ELKONITE® 40S Infiltrated Tungsten Silver contact material ASTM B631
For arcing and current carrying electrical contacts.Information provided by CMW Inc.
Thermal Conductivity 180 W/m-K
1250 BTU-in/hr-ft²-°F
Typical
Ceramic Process Systems AlSiC-10, 54 vol% SiC
Aluminum alloy A356.2 used. Hermeticity < 1x109 atm-cc/s He.CPS fabricates AlSiC by preparing an SiC preform which is subsequently infiltrated by molten aluminum metal. After infiltration, compone..
Thermal Conductivity 180 W/m-K
1250 BTU-in/hr-ft²-°F
Ceramic Process Systems AlSiC-8, 70 vol% SiC
Aluminum alloy A356.2 used. Hermeticity < 1x109 atm-cc/s He.CPS fabricates AlSiC by preparing an SiC preform which is subsequently infiltrated by molten aluminum metal. After infiltration, compone..
Thermal Conductivity 180 W/m-K
1250 BTU-in/hr-ft²-°F
Ametek Tungsten-Copper Composites AWC 8812
Information supplied by Ametek Specialty Metal Products.The material is available as finished parts with the following maximum dimensions:Width: 6 inches (152 mm)Thickness: 0.150 inches (3.8 mm)Leng..
Thermal Conductivity 180 W/m-K

@Temperature 20.0 - 100 °C
1250 BTU-in/hr-ft²-°F

@Temperature 68.0 - 212 °F
ASTM-C408
CeramTec CeramCool® Alunit® Aluminum Nitride
CeramCool® is a metallized ceramic heat-sink for high power applications demonstrated by high power LED-systems. CeramCool® material characteristics: electrical insulation, high volume resistivit..
Thermal Conductivity 180 W/m-K
1250 BTU-in/hr-ft²-°F
Typical
Ceramic Process Systems AlSiC-9, 63 vol% SiC
Aluminum alloy A356.2 used. Hermeticity < 1x109 atm-cc/s He.CPS fabricates AlSiC by preparing an SiC preform which is subsequently infiltrated by molten aluminum metal. After infiltration, compone..
Copyright © lookpolymers.com All Rights Reserved