Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 180 W/m-K | 1250 BTU-in/hr-ft²-°F | |
IBC Advanced Alloys Beralcast® 191 Beryllium-Aluminum Alloy This alloy consists of 65% Be and 35% Al (by weight) and is used primarily for moderate strength cast electronic and thermal packaging applications. BeAl-191 also provides a unique capability for se.. |
|||
Thermal Conductivity | 180 W/m-K | 1250 BTU-in/hr-ft²-°F | Longitudinal |
IBC Advanced Alloys Beralcast® 310 Beryllium-Aluminum Alloy This alloy, a metal matrix composite, consisting of between 60 and 70% Be (by weight) is a wrought product offered by IBC Engineered Materials to be used in the process of manufacturing extrusions f.. |
|||
Thermal Conductivity | 180 - 190 W/m-K | 1250 - 1320 BTU-in/hr-ft²-°F | z direction |
MarkeTech Cu/Mo/Cu 1:3:1 Laminated Sheet Cu/MoCu sheets have very high in-plane thermal conductivity provide by layers of Cu and low CTEs provided by the inner layer of molybdenum. These laminated sheets spread heat from a concentrated hea.. |
|||
Thermal Conductivity | 180 - 190 W/m-K | 1250 - 1320 BTU-in/hr-ft²-°F | |
MarkeTech W90Cu Tungsten/Copper Heat Sink Material WCu composites are made by vacuum infiltration of uniform controlled porous blocks of tungsten with molten copper. This results in a material with an interconnected Cu matrix that has high thermal c.. |
|||
Thermal Conductivity | 180 W/m-K | 1250 BTU-in/hr-ft²-°F | |
Sapco Aluminum Nitride Information provided by Sapco. |
|||
Thermal Conductivity | 180 W/m-K | 1250 BTU-in/hr-ft²-°F | ASTM E1461 |
M Cubed Technologies SSC-802 Reaction-Bonded Silicon Carbide Medium-grained reaction-bonded SiC for high wear applications. Bullnoses, fan liners, hydrocyclone liners, etc. Can be cast into very large shapes (greater than 4 ft. square, 5-6 inches thick)Info.. |
|||
Thermal Conductivity | 180 W/m-K | 1250 BTU-in/hr-ft²-°F | DIN EN 821-2 / ASTM-C408 |
CeramTec Alunit® Aluminum Nitride Alunit® offers an extremely high thermal conductivity of 180 W/mK and outstanding electrical insulation properties. The thermal expansion coefficient of this material is comparable to silicon. Its .. |
|||
Thermal Conductivity | 180 W/m-K | 1250 BTU-in/hr-ft²-°F | Casting |
CMW® 100 Copper Alloy CMW® 100 material is a heat treatable, high strength, high conductivity copper base alloy. Its properties are a combination of highest strength and hardness with relatively high electrical and ther.. |
|||
Thermal Conductivity | 180 W/m-K | 1250 BTU-in/hr-ft²-°F | |
CMW® ELKONITE® 40S Infiltrated Tungsten Silver contact material ASTM B631 For arcing and current carrying electrical contacts.Information provided by CMW Inc. |
|||
Thermal Conductivity | 180 W/m-K | 1250 BTU-in/hr-ft²-°F | Typical |
Ceramic Process Systems AlSiC-10, 54 vol% SiC Aluminum alloy A356.2 used. Hermeticity < 1x109 atm-cc/s He.CPS fabricates AlSiC by preparing an SiC preform which is subsequently infiltrated by molten aluminum metal. After infiltration, compone.. |
|||
Thermal Conductivity | 180 W/m-K | 1250 BTU-in/hr-ft²-°F | |
Ceramic Process Systems AlSiC-8, 70 vol% SiC Aluminum alloy A356.2 used. Hermeticity < 1x109 atm-cc/s He.CPS fabricates AlSiC by preparing an SiC preform which is subsequently infiltrated by molten aluminum metal. After infiltration, compone.. |
|||
Thermal Conductivity | 180 W/m-K | 1250 BTU-in/hr-ft²-°F | |
Ametek Tungsten-Copper Composites AWC 8812 Information supplied by Ametek Specialty Metal Products.The material is available as finished parts with the following maximum dimensions:Width: 6 inches (152 mm)Thickness: 0.150 inches (3.8 mm)Leng.. |
|||
Thermal Conductivity | 180 W/m-K @Temperature 20.0 - 100 °C |
1250 BTU-in/hr-ft²-°F @Temperature 68.0 - 212 °F |
ASTM-C408 |
CeramTec CeramCool® Alunit® Aluminum Nitride CeramCool® is a metallized ceramic heat-sink for high power applications demonstrated by high power LED-systems. CeramCool® material characteristics: electrical insulation, high volume resistivit.. |
|||
Thermal Conductivity | 180 W/m-K | 1250 BTU-in/hr-ft²-°F | Typical |
Ceramic Process Systems AlSiC-9, 63 vol% SiC Aluminum alloy A356.2 used. Hermeticity < 1x109 atm-cc/s He.CPS fabricates AlSiC by preparing an SiC preform which is subsequently infiltrated by molten aluminum metal. After infiltration, compone.. |