Sapco Aluminum Nitride

Category Ceramic , Nitride
Manufacturer Sapco
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sapco Aluminum Nitride.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Sapco.
Physical Properties Metric English Comments
Density 3.26 g/cc
0.118 lb/in³
Open Porosity 0.00 %
0.00 %
Mechanical Properties Metric English Comments
Modulus of Elasticity 308 GPa
44700 ksi
Thermal Properties Metric English Comments
CTE, linear 3.90 µm/m-°C

@Temperature 20.0 °C
2.17 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 180 W/m-K
1250 BTU-in/hr-ft²-°F
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
Dielectric Constant 8.9

@Frequency 1e+6 Hz
8.9

@Frequency 1e+6 Hz
Dielectric Strength 10.0 kV/mm
254 kV/in
AC