Thermal Properties Metric English Comments
Thermal Conductivity 21.8 W/m-K

@Temperature 600 °C
151 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Haynes HR-160® alloy plate, aged 1000 hours at 649°C (1200°F)
Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an..
Thermal Conductivity 21.8 W/m-K

@Temperature 600 °C
151 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Haynes HR-160® alloy plate, aged 4000 hours at 649°C (1200°F)
Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an..
Thermal Conductivity 21.8 W/m-K

@Temperature 600 °C
151 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Haynes HR-160® alloy, annealed plate
Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an..
Thermal Conductivity 21.8 W/m-K

@Temperature 600 °C
151 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Haynes HR-160® alloy, plate, aged 1000 hours at 760°C (1400°F)
Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an..
Thermal Conductivity 21.8 W/m-K

@Temperature 600 °C
151 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Haynes HR-160® alloy, plate, aged 1000 hours at 871°C (1600°F)
Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an..
Thermal Conductivity 21.8 W/m-K

@Temperature 600 °C
151 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Haynes HR-160® alloy, plate, aged 4000 hours at 760°C (1400°F)
Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an..
Thermal Conductivity 21.8 W/m-K

@Temperature 600 °C
151 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Haynes HR-160® alloy, plate, aged 4000 hours at 871°C (1600°F)
Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an..
Thermal Conductivity 21.8 W/m-K

@Temperature 600 °C
151 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Haynes HR-160® alloy, plate, aged 8000 hours at 760°C (1400°F)
Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an..
Thermal Conductivity 21.8 W/m-K

@Temperature 600 °C
151 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Haynes HR-160® alloy, plate, aged 8000 hours at 871°C (1600°F)
Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an..
Thermal Conductivity 21.8 W/m-K

@Temperature 600 °C
151 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Haynes HR-160® alloy plate, aged 8000 hours at 649°C (1200°F)
Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an..
Thermal Conductivity 21.8 W/m-K
151 BTU-in/hr-ft²-°F
Special Metals MONEL® Alloy 400
A nickel-copper alloy with high strength and excellent corrosion resistance in a range of media including sea water, hydrofluoric acid, sulfuric acid, and alkalis. Used for marine engineering, chem..
Thermal Conductivity 21.8 W/m-K
151 BTU-in/hr-ft²-°F
Special Metals MONEL® Alloy R-405
The free-machining version of MONEL alloy 400. A controlled amount of sulfur is added to the alloy to provide sulfide inclusions that act as chip breakers during machining. Other characteristics a..