Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Special Metals MONEL® Alloy R-405

Category Metal , Nonferrous Metal , Nickel Alloy , Superalloy
Manufacturer Special Metals (includes the former Inco Alloys International Inc.)
Trade Name MONEL®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Special Metals MONEL® Alloy R-405.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The free-machining version of MONEL alloy 400. A controlled amount of sulfur is added to the alloy to provide sulfide inclusions that act as chip breakers during machining. Other characteristics are essentially the same as those of MONEL alloy 400. Used for meter and valve parts, fasteners, and screw-machine products. Standard product forms are round, hexagon, flats, and wire.Data provided by the manufacturer, Special Metals.
Physical Properties Metric English Comments
Density 8.80 g/cc
0.318 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 550 MPa
79800 psi
Annealed
Tensile Strength, Yield 240 MPa

@Strain 0.200 %
34800 psi

@Strain 0.200 %
Annealed
Elongation at Break 40 %
40 %
Annealed
Thermal Properties Metric English Comments
CTE, linear 13.7 µm/m-°C

@Temperature 20.0 - 100 °C
7.61 µin/in-°F

@Temperature 68.0 - 212 °F
Specific Heat Capacity 0.427 J/g-°C
0.102 BTU/lb-°F
Thermal Conductivity 21.8 W/m-K
151 BTU-in/hr-ft²-°F
Melting Point 1300 - 1350 °C
2370 - 2460 °F
Solidus 1300 °C
2370 °F
Liquidus 1350 °C
2460 °F
Component Elements Properties Metric English Comments
Carbon, C <= 0.30 %
<= 0.30 %
Copper, Cu 28 - 34 %
28 - 34 %
Iron, Fe <= 2.5 %
<= 2.5 %
Manganese, Mn <= 2.0 %
<= 2.0 %
Nickel, Ni >= 63 %
>= 63 %
Silicon, Si <= 0.50 %
<= 0.50 %
Sulfur, S 0.025 - 0.060 %
0.025 - 0.060 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000510 ohm-cm
0.0000510 ohm-cm
Curie Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Copyright © lookpolymers.com All Rights Reserved