Special Metals MONEL® Alloy 400

Category Metal , Nonferrous Metal , Nickel Alloy , Superalloy
Manufacturer Special Metals (includes the former Inco Alloys International Inc.)
Trade Name MONEL®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Special Metals MONEL® Alloy 400.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A nickel-copper alloy with high strength and excellent corrosion resistance in a range of media including sea water, hydrofluoric acid, sulfuric acid, and alkalis. Used for marine engineering, chemical and hydrocarbon processing equipment, valves, pumps, shafts, fittings, fasteners, and heat exchangers. Standard product forms are round, hexagon, flats, forging stock, pipe, tube, plate, sheet, strip, and wire.Data provided by the manufacturer, Special Metals.
Physical Properties Metric English Comments
Density 8.80 g/cc
0.318 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 550 MPa
79800 psi
Annealed
450 MPa

@Temperature 425 °C
65300 psi

@Temperature 797 °F
Annealed prior to test
Tensile Strength, Yield 240 MPa
34800 psi
Annealed
170 MPa

@Temperature 425 °C
24700 psi

@Temperature 797 °F
Annealed prior to test
Elongation at Break 48 %
48 %
Annealed prior to test.
50 %

@Temperature 425 °C
50 %

@Temperature 797 °F
Annealed prior to test.
Thermal Properties Metric English Comments
CTE, linear 13.9 µm/m-°C

@Temperature 20.0 - 100 °C
7.72 µin/in-°F

@Temperature 68.0 - 212 °F
Specific Heat Capacity 0.427 J/g-°C
0.102 BTU/lb-°F
Thermal Conductivity 21.8 W/m-K
151 BTU-in/hr-ft²-°F
Melting Point 1300 - 1350 °C
2370 - 2460 °F
Solidus 1300 °C
2370 °F
Liquidus 1350 °C
2460 °F
Component Elements Properties Metric English Comments
Carbon, C <= 0.30 %
<= 0.30 %
Copper, Cu 28 - 34 %
28 - 34 %
Iron, Fe <= 2.5 %
<= 2.5 %
Manganese, Mn <= 2.0 %
<= 2.0 %
Nickel, Ni >= 63 %
>= 63 %
Including Cobalt
Silicon, Si <= 0.50 %
<= 0.50 %
Sulfur, S <= 0.024 %
<= 0.024 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000547 ohm-cm
0.0000547 ohm-cm
Curie Temperature 20.0 - 50.0 °C
68.0 - 122 °F