Thermal Properties Metric English Comments
Thermal Conductivity 1.00 - 2.00 W/m-K
6.94 - 13.9 BTU-in/hr-ft²-°F
Through Plane; ASTM E1461
PolyOne Trilliant™ HC HC0200-5001 XR Grey Thermoplastic Elastomer (TPE)
The Trilliant® specialty compounds offer a complete system of specialty engineered materials, certified processes, services and technical support that enable healthcare OEM's to get to market ahead..
Thermal Conductivity 1.50 - 2.00 W/m-K
10.4 - 13.9 BTU-in/hr-ft²-°F
ASTM E1461
PolyOne Trilliant™ HC HC6200-5002 XR Grey Polyamide 12 (Nylon 12)
The Trilliant® specialty compounds offer a complete system of specialty engineered materials, certified processes, services and technical support that enable healthcare OEM's to get to market ahead..
Thermal Conductivity 1.00 - 2.00 W/m-K
6.94 - 13.9 BTU-in/hr-ft²-°F
ASTM C177
PolyOne Therma-Tech™ SFC-5000 TC Polyphenylene Sulfide (PPS)  (discontinued **)
Therma-Tech™ Thermal Management Compounds have been engineered to combine the heat transfer and cooling capabilities of metals with the design freedom, weight reduction and cost advantages of therm..