Thermal Properties Metric English Comments
Thermal Conductivity 0.0400 W/m-K
0.278 BTU-in/hr-ft²-°F
MarkeTech Carbon Aerogel
Data provided by the supplier, MarkeTech International.Availability: Paper Sheets: 85 x 250 mm; Random Pieces 0.5-20 mm; Granules and Powder.Resorcinol Formaldehyde and Silica Aerogels are also list..
Thermal Conductivity 0.0400 W/m-K
0.278 BTU-in/hr-ft²-°F
DIN 52612
Lehmann & Voss LUVOCOM® AC-80/TF/22/BK Polyacetal-copolymer, with PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl..
Thermal Conductivity 0.0400 W/m-K
0.278 BTU-in/hr-ft²-°F
ASTM C518
SABIC Innovative Plastics ULTEM Foam XP110 PEI
ULTEM foam is a polyetherimide based thermoplastic foam with excellent flame, smoke and toxicity performance. The material combines a high strength to weight ratio with low moisture absorption. The ..
Thermal Conductivity 0.0400 W/m-K
0.278 BTU-in/hr-ft²-°F
mean temp of 10°C; ISO 8302 1991
Zotefoams Plastazote® LD15FM Low Density Polyethylene Foam, Flame Retarded
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..
Thermal Conductivity 0.0400 W/m-K
0.278 BTU-in/hr-ft²-°F
DuPont™ Kevlar® 29 Aramid Fiber
1500 Denier; 1000 Filaments. Kevlar® 29 yarns are used in ballistic applications, ropes and cables, protective apparel such as cut-resistant gloves, in life protection uses such as helmets, vehicu..
Thermal Conductivity 0.0400 W/m-K
0.278 BTU-in/hr-ft²-°F
DuPont™ Kevlar® 49 Aramid Fiber
1140 Denier; 768 Filaments. Kevlar® 49 is a high-modulus type used primarily in fiber optic cable, textile processing, plastic reinforcement, ropes, cables, and composites for marine sporting good..
Thermal Conductivity 0.0400 W/m-K
0.278 BTU-in/hr-ft²-°F
DIN 52612
BASF Neopolen® P 9035 0.06 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 9035 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9035.Note: In order to mea..
Thermal Conductivity 0.0400 W/m-K
0.278 BTU-in/hr-ft²-°F
DIN 52612
BASF Neopolen® P 9225 K 0.06 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 9225 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9225 K.Note: In order to..
Thermal Conductivity 0.0400 W/m-K
0.278 BTU-in/hr-ft²-°F
DIN 52612
BASF Neopolen® P 9230 A 0.07 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 9230 A is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 A.Note: In order to..
Thermal Conductivity 0.0400 W/m-K
0.278 BTU-in/hr-ft²-°F
DIN 52612
BASF Neopolen® P 9435 0.06 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 9435 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9435.Note: In order to mea..
Thermal Conductivity 0.0400 W/m-K
0.278 BTU-in/hr-ft²-°F
Moisture Content: 12%
BASF Styrodur® 3035 CS Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Thermal Conductivity 0.0400 W/m-K

@Thickness 180 mm
0.278 BTU-in/hr-ft²-°F

@Thickness 7.09 in
DIN EN 13164
BASF Styrodur® 3035 CS Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Thermal Conductivity 0.0400 W/m-K
0.278 BTU-in/hr-ft²-°F
Moisture Content: 12%
BASF Styrodur® 4000 CS Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Thermal Conductivity 0.0400 W/m-K
0.278 BTU-in/hr-ft²-°F
Moisture Content: 12%
BASF Styrodur® 5000 CS Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Thermal Conductivity 0.0400 W/m-K
0.278 BTU-in/hr-ft²-°F
ISO 8301
3A Composites Core Materials AIREX® R82.110 High Performance Structural Foam
AIREX® R82 is a closed-cell, thermoplastic polymer foam that combines outstanding fire resistance with low smoke and toxicity, along with excellent dielectric properties. It has a good strength to ..
Thermal Conductivity 0.0400 - 0.310 W/m-K
0.278 - 2.15 BTU-in/hr-ft²-°F
Average value: 0.203 W/m-K Grade Count:8
Overview of materials for Acetal Copolymer, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, PTFE Filled". Each property range of values reported is minimum and maximum values of ..
Thermal Conductivity 0.0400 W/m-K
0.278 BTU-in/hr-ft²-°F
DIN 52612
BASF Neopolen® P 9230 D 0.07 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 9230 D is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 D.Note: In order to..
Thermal Conductivity 0.0400 W/m-K
0.278 BTU-in/hr-ft²-°F
DIN 52612
BASF Neopolen® P 9230 K 0.06 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 9230 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 K.Note: In order to..
Thermal Conductivity 0.0400 W/m-K
0.278 BTU-in/hr-ft²-°F
DIN 52612
BASF Neopolen® P 9235 0.06 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 9235 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9235.Note: In order to mea..
Thermal Conductivity 0.0400 W/m-K
0.278 BTU-in/hr-ft²-°F
DIN 52612
BASF Neopolen® P 9255 0.06 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 9255 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9255.Note: In order to mea..
Thermal Conductivity 0.0400 W/m-K
0.278 BTU-in/hr-ft²-°F
Moisture Content: 12%
BASF Styrodur® 2500 C Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Thermal Conductivity 0.0400 W/m-K
0.278 BTU-in/hr-ft²-°F
Moisture Content: 12%
BASF Styrodur® 2800 C Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Thermal Conductivity 0.0400 W/m-K
0.278 BTU-in/hr-ft²-°F
Moisture Content: 12%
BASF Styrodur® 3035 CN Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..