Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.0400 W/m-K | 0.278 BTU-in/hr-ft²-°F | |
MarkeTech Carbon Aerogel Data provided by the supplier, MarkeTech International.Availability: Paper Sheets: 85 x 250 mm; Random Pieces 0.5-20 mm; Granules and Powder.Resorcinol Formaldehyde and Silica Aerogels are also list.. |
|||
Thermal Conductivity | 0.0400 W/m-K | 0.278 BTU-in/hr-ft²-°F | DIN 52612 |
Lehmann & Voss LUVOCOM® AC-80/TF/22/BK Polyacetal-copolymer, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl.. |
|||
Thermal Conductivity | 0.0400 W/m-K | 0.278 BTU-in/hr-ft²-°F | ASTM C518 |
SABIC Innovative Plastics ULTEM Foam XP110 PEI ULTEM foam is a polyetherimide based thermoplastic foam with excellent flame, smoke and toxicity performance. The material combines a high strength to weight ratio with low moisture absorption. The .. |
|||
Thermal Conductivity | 0.0400 W/m-K | 0.278 BTU-in/hr-ft²-°F | mean temp of 10°C; ISO 8302 1991 |
Zotefoams Plastazote® LD15FM Low Density Polyethylene Foam, Flame Retarded Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Thermal Conductivity | 0.0400 W/m-K | 0.278 BTU-in/hr-ft²-°F | |
DuPont™ Kevlar® 29 Aramid Fiber 1500 Denier; 1000 Filaments. Kevlar® 29 yarns are used in ballistic applications, ropes and cables, protective apparel such as cut-resistant gloves, in life protection uses such as helmets, vehicu.. |
|||
Thermal Conductivity | 0.0400 W/m-K | 0.278 BTU-in/hr-ft²-°F | |
DuPont™ Kevlar® 49 Aramid Fiber 1140 Denier; 768 Filaments. Kevlar® 49 is a high-modulus type used primarily in fiber optic cable, textile processing, plastic reinforcement, ropes, cables, and composites for marine sporting good.. |
|||
Thermal Conductivity | 0.0400 W/m-K | 0.278 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Neopolen® P 9035 0.06 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9035 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9035.Note: In order to mea.. |
|||
Thermal Conductivity | 0.0400 W/m-K | 0.278 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Neopolen® P 9225 K 0.06 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9225 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9225 K.Note: In order to.. |
|||
Thermal Conductivity | 0.0400 W/m-K | 0.278 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Neopolen® P 9230 A 0.07 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9230 A is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 A.Note: In order to.. |
|||
Thermal Conductivity | 0.0400 W/m-K | 0.278 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Neopolen® P 9435 0.06 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9435 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9435.Note: In order to mea.. |
|||
Thermal Conductivity | 0.0400 W/m-K | 0.278 BTU-in/hr-ft²-°F | Moisture Content: 12% |
BASF Styrodur® 3035 CS Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0400 W/m-K @Thickness 180 mm |
0.278 BTU-in/hr-ft²-°F @Thickness 7.09 in |
DIN EN 13164 |
BASF Styrodur® 3035 CS Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0400 W/m-K | 0.278 BTU-in/hr-ft²-°F | Moisture Content: 12% |
BASF Styrodur® 4000 CS Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0400 W/m-K | 0.278 BTU-in/hr-ft²-°F | Moisture Content: 12% |
BASF Styrodur® 5000 CS Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0400 W/m-K | 0.278 BTU-in/hr-ft²-°F | ISO 8301 |
3A Composites Core Materials AIREX® R82.110 High Performance Structural Foam AIREX® R82 is a closed-cell, thermoplastic polymer foam that combines outstanding fire resistance with low smoke and toxicity, along with excellent dielectric properties. It has a good strength to .. |
|||
Thermal Conductivity | 0.0400 - 0.310 W/m-K | 0.278 - 2.15 BTU-in/hr-ft²-°F | Average value: 0.203 W/m-K Grade Count:8 |
Overview of materials for Acetal Copolymer, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, PTFE Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Thermal Conductivity | 0.0400 W/m-K | 0.278 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Neopolen® P 9230 D 0.07 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9230 D is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 D.Note: In order to.. |
|||
Thermal Conductivity | 0.0400 W/m-K | 0.278 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Neopolen® P 9230 K 0.06 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9230 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 K.Note: In order to.. |
|||
Thermal Conductivity | 0.0400 W/m-K | 0.278 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Neopolen® P 9235 0.06 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9235 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9235.Note: In order to mea.. |
|||
Thermal Conductivity | 0.0400 W/m-K | 0.278 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Neopolen® P 9255 0.06 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9255 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9255.Note: In order to mea.. |
|||
Thermal Conductivity | 0.0400 W/m-K | 0.278 BTU-in/hr-ft²-°F | Moisture Content: 12% |
BASF Styrodur® 2500 C Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0400 W/m-K | 0.278 BTU-in/hr-ft²-°F | Moisture Content: 12% |
BASF Styrodur® 2800 C Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0400 W/m-K | 0.278 BTU-in/hr-ft²-°F | Moisture Content: 12% |
BASF Styrodur® 3035 CN Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |