Material Notes:
ULTEM foam is a polyetherimide based thermoplastic foam with excellent flame, smoke and toxicity performance. The material combines a high strength to weight ratio with low moisture absorption. The foam also possesses excellent dielectric properties. ULTEM foam is targeted at applications where structural fire performance, radar transparency, or extreme hot or cold environments are required. ULTEM foam is thermoformable and compatible with phenolic pre-pregs. Information on processing or secondary operations is available upon request.
Physical Properties Metric English Comments
Density 0.110 g/cc
0.00397 lb/in³
ASTM D1622
Water Absorption 4.0 %
4.0 %
ASTM C272
Mechanical Properties Metric English Comments
Tensile Strength 2.10 MPa
305 psi
ASTM D638
Tensile Modulus 0.0400 GPa
5.80 ksi
in plane; ASTM D638
Compressive Strength 1.70 MPa
247 psi
perpendicular to plane; ASTM D1621
Compressive Modulus 0.103 GPa
14.9 ksi
ASTM D1621
Shear Modulus 0.0240 GPa
3.48 ksi
ASTM C273
Shear Strength 1.40 MPa
203 psi
ASTM C273
Izod Impact, Unnotched (ISO) 0.900 kJ/m²
0.428 ft-lb/in²
ISO R179
Thermal Properties Metric English Comments
Thermal Conductivity 0.0400 W/m-K
0.278 BTU-in/hr-ft²-°F
ASTM C518
Descriptive Properties Value Comments
Insulation Radiant Panel PASSES
FAR 25.856
OSU total heat release (2 minute test) <55kW-min/m^2
FAR 25.853
OSU peak heat release rate (5 minute test) <55kW/m^2
FAR 25.853
Smoke Density <10Ds
FAR 25.853
Smoke Toxicity PASSES
OEM BSS
PASSES
OEM ABD
Vertical Burn at 60 Seconds PASSES
FAR 25.853