Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 162 µm/m-°C

@Temperature -40.0 - 149 °C
90.0 µin/in-°F

@Temperature -40.0 - 300 °F
ASTM E831
Quadrant EPP TIVAR® 88 W/BurnGuard, Flame Retardant Lining Material (ASTM Product Data Sheet)
Promotes reliable, steady bulk material flow Abrasion-, chemical- and corrosion-resistant Low coefficient of friction No moisture absorption Reduces or eliminates arching, ratholing and erractic fl..
CTE, linear 162 - 216 µm/m-°C

@Temperature 20.0 °C
90.0 - 120 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Arkema Group Kynar Flex® 2950 PVDF Copolymer  (discontinued **)
Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry..
CTE, linear 162 µm/m-°C

@Temperature 20.0 °C
90.0 µin/in-°F

@Temperature 68.0 °F
3M Dyneon™ CC604 PTFE, 20% Fiberglass Filled  (discontinued **)
Product Form: White, pelletized free-flowing powder. Applications include bearings, valve seats, seals.Data provided by Dyneon.
CTE, linear 162 µm/m-°C

@Temperature 20.0 °C
90.0 µin/in-°F

@Temperature 68.0 °F
3M Dyneon™ CC607 PTFE 35% Fiberglass Filled  (discontinued **)
Product Form: White, pelletized free-flowing powder. Applications include bearings, valve seats, seals.Data provided by Dyneon.
CTE, linear 162 µm/m-°C

@Temperature 20.0 °C
90.0 µin/in-°F

@Temperature 68.0 °F
3M Dyneon™ CC698 PTFE 20% Fiberglass/Carbon Filled  (discontinued **)
Product Form: Black, pelletized powder. Applications include valve seats.Data provided by Dyneon.
CTE, linear 162 µm/m-°C

@Temperature 20.0 °C
90.0 µin/in-°F

@Temperature 68.0 °F
ASTM D-696
Saint-Gobain Norton® ECTFE Fluoropolymer Film
Features/Benefits:Outstanding release propertiesPerformance from -200°C (-328°F) to 165°C (330°F)High dielectric strengthExcellent chemical, radiation, weather and abrasion resistanceNon..
CTE, linear 162 µm/m-°C

@Temperature 20.0 °C
90.0 µin/in-°F

@Temperature 68.0 °F
Trelleborg Emerson & Cuming Stycast® 4952/25 Two-Component Silicone High Service Temp Encapsulant
Features and Typical ApplicationsAbility to withstand high temperatures, thermal shock, and chemical exposure. These products are designed for heat generating electronic devices which operate in har..
CTE, linear 162 µm/m-°C

@Temperature -80.0 - -30.0 °C
90.0 µin/in-°F

@Temperature -112 - -22.0 °F
ASTM D696
Lubrizol Pellethane® 2363-90AE Thermoplastic Polyurethane Elastomer
Feature: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009.
CTE, linear 162 µm/m-°C
90.0 µin/in-°F
BCC Products BC 100 Medium Cyanoacrylate Adhesive
BC100 Medium, like its name in the medium viscosity version of cyanoacrylate adhesive that has become most popular in the super bonding applications. A 12 second fixture bond makes the BC100 the fas..
CTE, linear 162 µm/m-°C
90.0 µin/in-°F
BCC Products BC 100 Thin Cyanoacrylate Adhesive
BC100 Thin is a low viscosity material ideal for bonding larger areas. BC100 Thin has a 20 second fixture cure and able to fill gaps of .002” wide. BC100 Thin is perfectly designed for bonding plas..
CTE, linear 162 µm/m-°C
90.0 µin/in-°F
BCC Products BC 100 Thick Cyanoacrylate Adhesive
BC100 Thick is the slow and thickest member of the BCC Products line of cyanoacrylate adhesive. Excellent for gap filling the BC100 Thick has a 30 second fixture time allowing for the material to f..
CTE, linear 162 - 216 µm/m-°C
90.0 - 120 µin/in-°F
ASTM D696
Arkema Group KYNAR FLEX® 2750-01 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Very flexible, lubricated. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..