Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

BCC Products BC 100 Medium Cyanoacrylate Adhesive

Category Polymer , Adhesive , Thermoset , Acrylic/Cyanoacrylate Adhesive
Manufacturer BCC Products
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BCC Products BC 100 Medium Cyanoacrylate Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
BC100 Medium, like its name in the medium viscosity version of cyanoacrylate adhesive that has become most popular in the super bonding applications. A 12 second fixture bond makes the BC100 the fastest in our family of cyanoacrylates. Excellent for bonding rough and porous surfaces BC100 meets Military specification MLLA 46050 Type II Class II. Perfect for industrial manufacturing and repair applications, you can bond with speed. BONDING SCHEDULES: Plastics: 2-5 seconds, Rubber:
Physical Properties Metric English Comments
Brookfield Viscosity 80 - 120 cP

@Temperature 25.0 °C
80 - 120 cP

@Temperature 77.0 °F
Brookfield LVF, Spindle 1-60 RPM
Mechanical Properties Metric English Comments
Shear Strength >= 10.0 MPa
>= 1450 psi
ABS; ASTM D1002/DIN 53283
>= 12.0 MPa
>= 1740 psi
polycarbonate; ASTM D1002/DIN 53283
>= 18.0 MPa
>= 2610 psi
etched aluminum; ASTM D1002/DIN 53283
>= 20.0 MPa
>= 2900 psi
grit blasted steel; ASTM D1002/DIN 53283
>= 22.0 MPa
>= 3190 psi
rubbers; ASTM D1002/DIN 53283
18.0 - 28.0 MPa
2610 - 4060 psi
tensile; ASTM D1002/DIN 53283
>= 25.0 MPa
>= 3630 psi
wood; ASTM D1002/DIN 53283
Thermal Properties Metric English Comments
CTE, linear 162 µm/m-°C
90.0 µin/in-°F
Thermal Conductivity 0.100 W/m-K
0.694 BTU-in/hr-ft²-°F
ASTM C177
Melting Point 160 - 170 °C
320 - 338 °F
Maximum Service Temperature, Air 80.0 °C
176 °F
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Glass Transition Temp, Tg 50.0 °C
122 °F
Electrical Properties Metric English Comments
Dielectric Strength 24.6 kV/mm
625 kV/in
Processing Properties Metric English Comments
Cure Time 0.016667 - 0.33333 min

@Temperature 24.0 °C
0.00027778 - 0.0055555 hour

@Temperature 75.2 °F
1440 min

@Temperature 24.0 °C
24.0 hour

@Temperature 75.2 °F
full cure
Descriptive Properties Value Comments
Gap Filling 0.2mm
Copyright © lookpolymers.com All Rights Reserved