Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

3M Dyneon™ CC607 PTFE 35% Fiberglass Filled  (discontinued **)

Category Polymer , Thermoplastic , Fluoropolymer , PTFE , Polytetrafluoroethylene (PTFE), Glass Filled, Molded
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Dyneon™ CC607 PTFE 35% Fiberglass Filled  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Form: White, pelletized free-flowing powder. Applications include bearings, valve seats, seals.Data provided by Dyneon.
Physical Properties Metric English Comments
Density 2.23 g/cc
0.0806 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore D 58
58
value after 15 sec; ASTM D2240
63
63
initial value; ASTM D2240
Tensile Strength, Ultimate 13.1 MPa
1900 psi
ASTM D4745
Elongation at Break 180 %
180 %
ASTM D4894
Flexural Yield Strength <= 18.0 MPa
<= 2610 psi
ASTM D790
Compressive Yield Strength 7.80 MPa
1130 psi
ASTM D695
Compressive Modulus 0.430 GPa
62.4 ksi
ASTM D695
Coefficient of Friction, Dynamic 0.36
0.36
ASTM D3702
Coefficient of Friction, Static 0.27
0.27
ASTM D3702
K (wear) Factor 142 x 10-8 mm³/N-M
70.6 x 10-10 in³-min/ft-lb-hr
at 5000 psi - fpm PV; ASTM D3702
Thermal Properties Metric English Comments
CTE, linear 162 µm/m-°C

@Temperature 20.0 °C
90.0 µin/in-°F

@Temperature 68.0 °F
Copyright © lookpolymers.com All Rights Reserved