Thermal Properties Metric English Comments
CTE, linear 8.50 µm/m-°C
4.72 µin/in-°F
Poco Graphite DFP-1C (Copper impregnated) Semiconductor Grade Graphite
Although it is impossible to identify differences between various grades of graphite by looking at them, each grade has a special set of characteristics and physical properties that determine their ..
CTE, linear 8.50 µm/m-°C
4.72 µin/in-°F
Poco Graphite Glassmate® LT Graphite
In very high wear situations, LT, with a hardness rating higher than GM material, will resist wear longer.
CTE, linear 8.50 µm/m-°C

@Temperature 20.0 °C
4.72 µin/in-°F

@Temperature 68.0 °F
Pyrotek Valcor® G Pre-Cast Shapes
ApplicationsBurner blocks Skimmer blocks Cover blocks Specialty blocks Plungers Stirrers Spouts Feeder tubes AdvantagesProven performance in molten glass contact applications Smooth surface finish d..
CTE, linear 8.50 µm/m-°C
4.72 µin/in-°F
at Set Pt.
Ferro EG 4010 Display Device
Glass Type: Pb-B-AL Typical Powder Form: VSD Typical Application: Dielectric Ferro's display sealing glasses and dielectrics are low-temperature lead glasses suitable for hermetic sealing and pas..
CTE, linear 8.50 - 8.90 µm/m-°C

@Temperature 20.0 - 100 °C
4.72 - 4.94 µin/in-°F

@Temperature 68.0 - 212 °F
MarkeTech Cu/Mo/Cu 1:2:1 Laminated Sheet
Cu/MoCu sheets have very high in-plane thermal conductivity provide by layers of Cu and low CTEs provided by the inner layer of molybdenum. These laminated sheets spread heat from a concentrated hea..
CTE, linear 8.50 µm/m-°C

@Temperature 20.0 °C
4.72 µin/in-°F

@Temperature 68.0 °F
MMCC Cu/Al2O3 Particulate Copper Matrix Composite
Cast, discontinuously reinforced aluminum matrix composite. May be fabricated by vacuum infiltration of the ceramic preform.Data provided by the manufacturer, Metal Matrix Cast Composites (MMCC).
CTE, linear 8.50 µm/m-°C

@Temperature 20.0 - 100 °C
4.72 µin/in-°F

@Temperature 68.0 - 212 °F
TIMET TIMETAL® 551 (Ti-4Al-4Mo-4Sn-0.5Si) Titanium Alloy;
High-Strength Forging AlloyIndustry Specifications: UK Aerospace Specifications BS TA.38, 39, 40, 41, 42.Features: TIMETAL 551 has high strength and is creep resistant up to 400°C. It has a simila..
CTE, linear 8.50 µm/m-°C

@Temperature 20.0 - 100 °C
4.72 µin/in-°F

@Temperature 68.0 - 212 °F
TIMET TIMETAL® 551 (Ti-4Al-4Mo-4Sn-0.5Si) Titanium Alloy; 25-100 mm
High-Strength Forging AlloyIndustry Specifications: UK Aerospace Specifications BS TA.38, 39, 40, 41, 42.Features: TIMETAL 551 has high strength and is creep resistant up to 400°C. It has a simila..
CTE, linear 8.50 µm/m-°C

@Temperature 25.0 - 1000 °C
4.72 µin/in-°F

@Temperature 77.0 - 1830 °F
ASTM C372
CoorsTek Alumina-Zirconia Composite, AZ-25
Information provided by CoorsTek.
CTE, linear 8.50 µm/m-°C

@Temperature 20.0 °C
4.72 µin/in-°F

@Temperature 68.0 °F
CMW® THERMKON® 83 Tungsten Copper parts
For matching CTE of semiconductor substrates while allowing high thermal transfer.Information provided by CMW Inc.
CTE, linear 8.50 µm/m-°C
4.72 µin/in-°F
Anderman Ceramics EA999 Sintered Alumina, 99.9%
Densely sintered alumina is characterized by: high strength and hardness, temperature stability, electrical insulation, and high wear resistance and corrosion resistance even at high temperatures. ..
CTE, linear 8.50 - 13.7 µm/m-°C
4.72 - 7.61 µin/in-°F
Anderman Ceramics EREY99 Yttrium Oxide
Rare earth refractory oxide ceramics exhibit very high thermal stability, wear resistance, and strength. They are widely used in applications above 3090 °F (1700 °C), nuclear, high performance met..