Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 8.50 µm/m-°C | 4.72 µin/in-°F | |
Poco Graphite DFP-1C (Copper impregnated) Semiconductor Grade Graphite Although it is impossible to identify differences between various grades of graphite by looking at them, each grade has a special set of characteristics and physical properties that determine their .. |
|||
CTE, linear | 8.50 µm/m-°C | 4.72 µin/in-°F | |
Poco Graphite Glassmate® LT Graphite In very high wear situations, LT, with a hardness rating higher than GM material, will resist wear longer. |
|||
CTE, linear | 8.50 µm/m-°C @Temperature 20.0 °C |
4.72 µin/in-°F @Temperature 68.0 °F |
|
Pyrotek Valcor® G Pre-Cast Shapes ApplicationsBurner blocks Skimmer blocks Cover blocks Specialty blocks Plungers Stirrers Spouts Feeder tubes AdvantagesProven performance in molten glass contact applications Smooth surface finish d.. |
|||
CTE, linear | 8.50 µm/m-°C | 4.72 µin/in-°F | at Set Pt. |
Ferro EG 4010 Display Device Glass Type: Pb-B-AL Typical Powder Form: VSD Typical Application: Dielectric Ferro's display sealing glasses and dielectrics are low-temperature lead glasses suitable for hermetic sealing and pas.. |
|||
CTE, linear | 8.50 - 8.90 µm/m-°C @Temperature 20.0 - 100 °C |
4.72 - 4.94 µin/in-°F @Temperature 68.0 - 212 °F |
|
MarkeTech Cu/Mo/Cu 1:2:1 Laminated Sheet Cu/MoCu sheets have very high in-plane thermal conductivity provide by layers of Cu and low CTEs provided by the inner layer of molybdenum. These laminated sheets spread heat from a concentrated hea.. |
|||
CTE, linear | 8.50 µm/m-°C @Temperature 20.0 °C |
4.72 µin/in-°F @Temperature 68.0 °F |
|
MMCC Cu/Al2O3 Particulate Copper Matrix Composite Cast, discontinuously reinforced aluminum matrix composite. May be fabricated by vacuum infiltration of the ceramic preform.Data provided by the manufacturer, Metal Matrix Cast Composites (MMCC). |
|||
CTE, linear | 8.50 µm/m-°C @Temperature 20.0 - 100 °C |
4.72 µin/in-°F @Temperature 68.0 - 212 °F |
|
TIMET TIMETAL® 551 (Ti-4Al-4Mo-4Sn-0.5Si) Titanium Alloy; High-Strength Forging AlloyIndustry Specifications: UK Aerospace Specifications BS TA.38, 39, 40, 41, 42.Features: TIMETAL 551 has high strength and is creep resistant up to 400°C. It has a simila.. |
|||
CTE, linear | 8.50 µm/m-°C @Temperature 20.0 - 100 °C |
4.72 µin/in-°F @Temperature 68.0 - 212 °F |
|
TIMET TIMETAL® 551 (Ti-4Al-4Mo-4Sn-0.5Si) Titanium Alloy; 25-100 mm High-Strength Forging AlloyIndustry Specifications: UK Aerospace Specifications BS TA.38, 39, 40, 41, 42.Features: TIMETAL 551 has high strength and is creep resistant up to 400°C. It has a simila.. |
|||
CTE, linear | 8.50 µm/m-°C @Temperature 25.0 - 1000 °C |
4.72 µin/in-°F @Temperature 77.0 - 1830 °F |
ASTM C372 |
CoorsTek Alumina-Zirconia Composite, AZ-25 Information provided by CoorsTek. |
|||
CTE, linear | 8.50 µm/m-°C @Temperature 20.0 °C |
4.72 µin/in-°F @Temperature 68.0 °F |
|
CMW® THERMKON® 83 Tungsten Copper parts For matching CTE of semiconductor substrates while allowing high thermal transfer.Information provided by CMW Inc. |
|||
CTE, linear | 8.50 µm/m-°C | 4.72 µin/in-°F | |
Anderman Ceramics EA999 Sintered Alumina, 99.9% Densely sintered alumina is characterized by: high strength and hardness, temperature stability, electrical insulation, and high wear resistance and corrosion resistance even at high temperatures. .. |
|||
CTE, linear | 8.50 - 13.7 µm/m-°C | 4.72 - 7.61 µin/in-°F | |
Anderman Ceramics EREY99 Yttrium Oxide Rare earth refractory oxide ceramics exhibit very high thermal stability, wear resistance, and strength. They are widely used in applications above 3090 °F (1700 °C), nuclear, high performance met.. |