Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 8.50 - 13.7 µm/m-°C | 4.72 - 7.61 µin/in-°F | |
Anderman Ceramics EREY99 Yttrium Oxide Rare earth refractory oxide ceramics exhibit very high thermal stability, wear resistance, and strength. They are widely used in applications above 3090 °F (1700 °C), nuclear, high performance met.. |