MMCC Cu/Al2O3 Particulate Copper Matrix Composite

Category Ceramic , Oxide , Aluminum Oxide , Metal , Metal Matrix Composite , Nonferrous Metal , Copper Alloy
Manufacturer Metal Matrix Cast Composites (MMCC)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MMCC Cu/Al2O3 Particulate Copper Matrix Composite.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Cast, discontinuously reinforced aluminum matrix composite. May be fabricated by vacuum infiltration of the ceramic preform.Data provided by the manufacturer, Metal Matrix Cast Composites (MMCC).
Physical Properties Metric English Comments
Density 6.00 g/cc
0.217 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 400 - 600 MPa
58000 - 87000 psi
Modulus of Elasticity 220 - 240 GPa
31900 - 34800 ksi
Youngs Modulus
Thermal Properties Metric English Comments
CTE, linear 8.50 µm/m-°C

@Temperature 20.0 °C
4.72 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 120 W/m-K
833 BTU-in/hr-ft²-°F