Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Axiall 7048A Rigid PVC, Extrusion

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Axiall
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall 7048A Rigid PVC, Extrusion.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Georgia Gulf 7048A is a general purpose rigid PVC profile extrusion compound designed for applications requiring the following properties: Impact Strength & ToughnessFlame RetardantColorabilityCertification by NSF Standards 51& 61Dimensional StabilityChemical ResistanceUV Color StabilityInformation provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.38 g/cc
1.38 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Rockwell R 112
112
ASTM D-785
Hardness, Shore D 80
80
ASTM D-2240
Tensile Strength, Yield 42.7 MPa
6200 psi
ASTM D-638
Tensile Modulus 2.86 GPa
415 ksi
ASTM D-638
Flexural Strength 77.2 MPa
11200 psi
ASTM D-790
Flexural Modulus 2.62 GPa
380 ksi
ASTM D-790
Izod Impact, Notched 9.61 J/cm
18.0 ft-lb/in
ASTM D-256
Tensile Impact Strength 151 kJ/m²
72.0 ft-lb/in²
ASTM D-1822
Thermal Properties Metric English Comments
CTE, linear 66.6 µm/m-°C

@Temperature 20.0 °C
37.0 µin/in-°F

@Temperature 68.0 °F
ASTM D-696
Deflection Temperature at 1.8 MPa (264 psi) 72.2 °C
162 °F
ASTM D-648
Flammability, UL94 V-0
V-0
At 0.03 inch
Descriptive Properties Value Comments
Cell Classification 14423433
ASTM D-4216
Users viewing this material also viewed the following: