Polymer Property : CTE, linear = 6.50 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 11.7 µm/m-°C
6.50 µin/in-°F
ASTM D696
Haysite Heatmeiser® H340 Platen Insulation
Haysite’s family of mold and platen insulation products are specially engineered fiberglass reinforced thermoset polyester composites which offer superior energy efficiency, temperature control..
CTE, linear 11.7 µm/m-°C

@Temperature 20.0 °C
6.50 µin/in-°F

@Temperature 68.0 °F
Goodfellow Tungsten 60/Copper 40 Alloy
Information provided by Goodfellow.
CTE, linear 11.7 µm/m-°C

@Temperature 20.0 - 100 °C
6.50 µin/in-°F

@Temperature 68.0 - 212 °F
Goodfellow Evanohm® Precision Resistance Nickel Alloy
Electrical resistance alloy with a very low temperature coefficient of resistivityInformation provided by Goodfellow.
CTE, linear 11.7 µm/m-°C

@Temperature 20.0 °C
6.50 µin/in-°F

@Temperature 68.0 °F
Aremco Ceramacast™ 584 High Temperature Potting & Casting Material Magnesia
Two-part, quick-set ceramic for small parts.
CTE, linear 11.7 µm/m-°C

@Temperature 21.1 - 204 °C
6.50 µin/in-°F

@Temperature 70.0 - 400 °F
Schmolz + Bickenbach Cryodur® 2363 (A-2) Cold Work Die Steel
Description: Cryodur® 2363 is a cold-work steel developed for an excellent combination of wear resistance and toughness and Supplied in the annealed conditionCharacteristics: Good wear resistance; ..