Material Notes:
Information provided by Goodfellow.
Physical Properties Metric English Comments
Density 13.0 g/cc
0.470 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength at Break 460 MPa
66700 psi
Thermal Properties Metric English Comments
CTE, linear 11.7 µm/m-°C

@Temperature 20.0 °C
6.50 µin/in-°F

@Temperature 68.0 °F
Specific Heat Capacity 0.240 J/g-°C
0.0574 BTU/lb-°F
Thermal Conductivity 228 W/m-K
1580 BTU-in/hr-ft²-°F
Component Elements Properties Metric English Comments
Copper, Cu 40 %
40 %
Tungsten, W 60 %
60 %