Thermal Properties Metric English Comments
CTE, linear 96.0 µm/m-°C

@Temperature -30.0 - 100 °C
53.3 µin/in-°F

@Temperature -22.0 - 212 °F
ASTM D696
LyondellBasell Hifaxâ„¢ ETA-3104HF Thermoplastic Olefin Resin
Key Features: medium melt flow, medium modulus thermoplastic elastomeric olefin resin, good impact and stiffness balance, good dimensional stability, good processabilityApplications: molded-in color..
CTE, linear 96.0 µm/m-°C
53.3 µin/in-°F
ISO 11359-2
Unitika A1030BRL PA6, Conditioned
Information provided by Unitika Ltd.
CTE, linear 96.0 µm/m-°C
53.3 µin/in-°F
ISO 11359-2
Unitika A1030BRL PA6, Dry
Information provided by Unitika Ltd.
CTE, linear 96.0 µm/m-°C
53.3 µin/in-°F
ISO 11359-2
Unitika A1030FR PA6, Conditioned
Information provided by Unitika Ltd.
CTE, linear 96.0 µm/m-°C
53.3 µin/in-°F
ISO 11359-2
Unitika A1030FR PA6, Dry
Information provided by Unitika Ltd.
CTE, linear 96.0 µm/m-°C
53.3 µin/in-°F
ISO 11359-2
Unitika A1030JR PA6, Conditioned
Information provided by Unitika Ltd.
CTE, linear 96.0 µm/m-°C
53.3 µin/in-°F
ISO 11359-2
Unitika A1030SR PA6, Dry
Information provided by Unitika Ltd.
CTE, linear 96.0 µm/m-°C
53.3 µin/in-°F
ISO 11359-2
Unitika A1030JR PA6, Dry
Information provided by Unitika Ltd.
CTE, linear 96.0 µm/m-°C
53.3 µin/in-°F
ISO 11359-2
Unitika A1030SR PA6, Conditioned
Information provided by Unitika Ltd.
CTE, linear 96.0 µm/m-°C
53.3 µin/in-°F
Below Tg
Epoxy Technology EPO-TEK® 354 High Temperature Epoxy
Product Description: EPO-TEK® 354 is a two component, high Tg epoxy designed for semiconductor packaging in medical, fiber optic and optoelectronic assemblies. It is an electrically and thermally i..
Copyright © lookpolymers.com All Rights Reserved