CTE, linear 86.0 µm/m-°C

@Thickness 2.00 mm,
Temperature -125 - 20.0 °C
47.8 µin/in-°F

@Thickness 0.0787 in,
Temperature -193 - 68.0 °F
ASTM E831-06
NeXolve UV Blocking Optionox® Polyimide Film/Coating
Highly UV durable with excellent weatherability and stability to ozone.Optinox® films and coatings are highly UV durable and exhibit excellent weathering durability, including very high stability ..
CTE, linear 86.0 - 370 µm/m-°C

@Temperature -40.0 - 85.0 °C
47.8 - 206 µin/in-°F

@Temperature -40.0 - 185 °F
Average value: 185 µm/m-°C Grade Count:5
Overview of materials for Polyvinylidinefluoride (PVDF), Molded/Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polyvinylidinefluoride (PVDF), Molded/Extruded". Each property range of values reported is minimum and m..
CTE, linear 86.0 µm/m-°C

@Temperature 20.0 °C
47.8 µin/in-°F

@Temperature 68.0 °F
ASTM E831
BASF Capron® 8224 HSL Nylon 6 (DAM)  (discontinued **)
Information provided by BASF Corporation.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line.
CTE, linear 86.0 µm/m-°C

@Temperature 20.0 °C
47.8 µin/in-°F

@Temperature 68.0 °F
ISO 11359
LG Chemical AF-320T ABS, Flame Retardant, High Impact, High Flow, Slim Wall
Information Provided by LG Chem
CTE, linear 86.0 µm/m-°C

@Temperature 40.0 - 130 °C
47.8 µin/in-°F

@Temperature 104 - 266 °F
TMA; ASTM E831
Plenco 1586 Polyester, Pellet, Injection Molded
PLENCO 01586 is a glass and mineral reinforced pelletized polyester molding compound offering excellent heat resistance and mechanical strength properties. This product is typically used for injecti..
CTE, linear 86.0 µm/m-°C
47.8 µin/in-°F
Above Tg
Tra-Con Tra-Bond 77-2LTC Low Temperature Cure SMD Adhesive
TRA-BOND 77-2LTC one component, solvent-free, insulative epoxy adhesive is designed to cure at temperatures as low as 80°C. This adhesive is specifically designed for attaching surface mounted devi..
CTE, linear 86.0 µm/m-°C

@Temperature 20.0 °C
47.8 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Devcon Plastic Steel® Putty (A) Epoxy
General Repair EpoxyComments: The original metal-filled epoxy putty used for hundreds of routine maintenance, production and tooling applications. Bonds to most metal, concrete and some plastics. ..
CTE, linear 86.0 µm/m-°C

@Temperature 20.0 °C
47.8 µin/in-°F

@Temperature 68.0 °F
Armstrong A-2/W Epoxy Adhesive
This off-white paste epoxy is a versatile adhesive systems. The choice of one of four recommended Activators (A, E, W or H-20) makes A-2 Adhesive an ideal choice for many applications. A-2 with Ac..
CTE, linear 86.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
47.8 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359
CENTROPLAST CENTROLAB HT Polypropylene Higher Temperatures
PP-HT is a semi-crystalline plastic, with high acid and chemical resistance and mechanical strength. Due to its high resistance to temperature, PP-HT-plastics are often used in medical technology as..