Material Notes:
Highly UV durable with excellent weatherability and stability to ozone.Optinox® films and coatings are highly UV durable and exhibit excellent weathering durability, including very high stability to ozone. Optinox® is available in rolls up to 60” wide, or in low-temperature curing liquids for coating applications. Both the film rolls and liquid coatings are available in three grades, outlined below.Optinox® rolls are provided either as a freestanding film, or permanently bonded to a PET backer. Additional thicknesses are also available upon request. Optinox® liquid curing resins are provided as a two-part curing system.Transparent Clear:UV cutoff at approximately 230 nm for a 2 mm film or coatingTransparent UV Blocking:UV cutoff at approximately 395 nm for a 2 mm film or coatingReflective White:Reflective White FilmInformation Provided by NeXolve Corporation.
Mechanical Properties Metric English Comments
Tensile Strength 41.0 MPa

@Thickness 0.0500 mm
5950 psi

@Thickness 0.00197 in
ASTM D882-02
Elongation at Break 95 %

@Thickness 0.0500 mm
95 %

@Thickness 0.00197 in
ASTM D882-02
Elongation at Yield 74 %

@Thickness 0.0500 mm
74 %

@Thickness 0.00197 in
ASTM D882-02
Modulus of Elasticity 0.960 GPa
139 ksi
ASTM D882-02
Thermal Properties Metric English Comments
CTE, linear 86.0 µm/m-°C

@Thickness 2.00 mm,
Temperature -125 - 20.0 °C
47.8 µin/in-°F

@Thickness 0.0787 in,
Temperature -193 - 68.0 °F
ASTM E831-06
Glass Transition Temp, Tg 29.0 °C
84.2 °F
DSC; ASTM E1356-03
Optical Properties Metric English Comments
Refractive Index 1.45

@Wavelength 549 nm
1.45

@Wavelength 549 nm
Abbe; ASTM D542-00
Transmission, Visible 0.86 %

@Thickness 0.0500 mm
0.86 %

@Thickness 0.00197 in
Solar Transmittivity; ASTM E903-96
Reflection Coefficient, Visible (0-1) 0.060

@Thickness 0.0500 mm
0.060

@Thickness 0.00197 in
Solar Reflectivity; ASTM E903-96
Descriptive Properties Value Comments
Applications Composites Protection
Conformal Coatings
Corrosion Resistance
Characteristics Extreme environment (high UV, ozone) durability
Flexible, tough conformal coating
High optical clarity
Long-term terrestrial weathering protection
Low temperature curing
Solar Absorptivity 0.07
2.0 mil thickness; ASTM E903-96