CTE, linear 3.90 µm/m-°C

@Temperature 20.0 °C
2.17 µin/in-°F

@Temperature 68.0 °F
Pyrotek Insural® 140 Insulating Refractory Shapes for Aluminum
Insural® 140 Precast Shapes are designed for the containment of molten aluminum in hot top modules (cross feeder) and trough/launder applications.AdvantagesNear zero expansion avoids gaps at the jo..
CTE, linear 3.90 µm/m-°C

@Temperature 20.0 °C
2.17 µin/in-°F

@Temperature 68.0 °F
Pyrotek O'-Sialon Non-Oxide Ceramic
O'-Sialon is a unique class of non-oxide ceramic which incorporates grains of silicon carbide held by a matrix of O'-Sialon. This results in a product that exhibits high strength at both ..
CTE, linear 3.90 µm/m-°C

@Temperature 20.0 - 300 °C
2.17 µin/in-°F

@Temperature 68.0 - 572 °F
ISO 7991
Schott Glass 8487 Borosilicate Glass
Borosilicate glass for sealing to tungsten Backlights, flash lamps, lamp bulbs, exhaust and flare bulbs The heavy metal content for the elements lead, cadmium, mercury, and hexavalent chromium is ..
CTE, linear 3.90 µm/m-°C

@Temperature 20.0 - 300 °C
2.17 µin/in-°F

@Temperature 68.0 - 572 °F
ISO 7991
Schott Glass 8687 Borosilicate Glass
Borosilicate glass for sealing to tungsten, defined UV absorption, stabilized against solarization Backlights The heavy metal content for the elements lead, cadmium, mercury, and hexavalent chromi..
CTE, linear 3.90 µm/m-°C

@Temperature 20.0 °C
2.17 µin/in-°F

@Temperature 68.0 °F
Sapco Aluminum Nitride
Information provided by Sapco.
CTE, linear 3.90 µm/m-°C
2.17 µin/in-°F
Tokuyama Shapal™ SH-50 Sintered Aluminum Nitride
Uniform, large sized pressed sintered aluminum nitride.
CTE, linear 3.90 µm/m-°C

@Temperature 25.0 - 1000 °C
2.17 µin/in-°F

@Temperature 77.0 - 1830 °F
ASTM C372
CoorsTek Nitrogen Bonded Silicon Carbide, SCNB
Thermal Shock Delta Tc = 400°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar..
CTE, linear 3.90 µm/m-°C

@Temperature 900 °C
2.17 µin/in-°F

@Temperature 1650 °F
COI Ceramics Nicalon™ HRV SiCO Ceramic Fiber
Description: The fiber is homogeneously composed of ultra-fine beta-SiC crystallites and an amorphous mixture of silicon, carbon, and oxygen. The fiber has excellent strength and modulus properties ..
CTE, linear 3.90 µm/m-°C

@Temperature 27.0 - 175 °C
2.17 µin/in-°F

@Temperature 80.6 - 347 °F
ASTM D696
3M 7995MP Hi-Performance Acrylic 200MP
This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materia..
Copyright © lookpolymers.com All Rights Reserved