Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

CoorsTek Nitrogen Bonded Silicon Carbide, SCNB

Category Ceramic , Carbide
Manufacturer CoorsTek
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CoorsTek Nitrogen Bonded Silicon Carbide, SCNB.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Thermal Shock Delta Tc = 400°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a sharp decrease in the flexural strength of the sample.Information provided by CoorsTek.
Physical Properties Metric English Comments
Density 2.60 g/cc
0.0939 lb/in³
ASTM C20
Water Absorption 8.0 %
8.0 %
ASTM C373
Mechanical Properties Metric English Comments
Modulus of Elasticity 152 GPa
22000 ksi
ASTM C848
Flexural Strength 48.0 MPa
6960 psi
ASTM F417
Compressive Strength 140 MPa
20300 psi
ASTM C773
Thermal Properties Metric English Comments
CTE, linear 3.90 µm/m-°C

@Temperature 25.0 - 1000 °C
2.17 µin/in-°F

@Temperature 77.0 - 1830 °F
ASTM C372
Thermal Conductivity 80.0 W/m-K
555 BTU-in/hr-ft²-°F
ASTM C408
Maximum Service Temperature, Air 1600 °C
2910 °F
No Load
Optical Properties Metric English Comments
Transmission, Visible 0.00 %
0.00 %
Users viewing this material also viewed the following: