Pyrotek O'-Sialon Non-Oxide Ceramic

Category Ceramic , Carbide
Manufacturer Pyrotek, Inc.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Pyrotek O'-Sialon Non-Oxide Ceramic.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
O'-Sialon is a unique class of non-oxide ceramic which incorporates grains of silicon carbide held by a matrix of O'-Sialon. This results in a product that exhibits high strength at both room temperature and working temperature. It also gives longer life meaning less change-overs and less down time. No expensive and time consuming coatings are required because O'-Sialon is non-wetting to molten aluminum and its alloys.ApplicationsDosing tubes Riser tubes Heater protection tubes Thermocouple Protection tubes AdvantagesExcellent oxidation resistance Non-wetting to aluminum and its alloys Good thermal shock Good abrasion resistance Chemically inert Information provided by Pyrotek.
Physical Properties Metric English Comments
Density 2.62 g/cc
0.0947 lb/in³
Open Porosity 13 - 20 %
13 - 20 %
Mechanical Properties Metric English Comments
Modulus of Rupture 0.160 GPa
23.2 ksi
Thermal Properties Metric English Comments
CTE, linear 3.90 µm/m-°C

@Temperature 20.0 °C
2.17 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 8.90 W/m-K

@Temperature 720 °C
61.8 BTU-in/hr-ft²-°F

@Temperature 1330 °F
Maximum Service Temperature, Air 1500 °C
2730 °F
Continuous
Component Elements Properties Metric English Comments
SiC 65 %