Thermal Properties Metric English Comments
CTE, linear 30.0 - 35.0 µm/m-°C
16.7 - 19.4 µin/in-°F
Polykemi
Polykemi AB POLYblend 45FS GF20 PC/ABS-Blend, Glass Fiber reinforced
Information provided by Polykemi AB
CTE, linear 15.0 - 35.0 µm/m-°C

@Temperature 50.0 - 100 °C
8.33 - 19.4 µin/in-°F

@Temperature 122 - 212 °F
longitudinal; ISO 11359-2
Raschig Group MELOPLAS® 150 MF
Wood flour-reinforced MF molding compound in dark colors. High surface hardness, high mechanical strength, good electrical properties. Self-extinguishing (V-O/1,6 according to UL 94), UL-listed. Fr..
CTE, linear 15.0 - 35.0 µm/m-°C

@Temperature 50.0 - 100 °C
8.33 - 19.4 µin/in-°F

@Temperature 122 - 212 °F
longitudinal; ISO 11359-2
Raschig Group MELOPLAS® 152 MF
Cellulose-reinforced MF molding compound in white and colored shades. Very good electrical properties, high surface hardness, good abrasion- and UV-stability, very good resistance to chemicals - al..
CTE, linear 15.0 - 35.0 µm/m-°C

@Temperature 50.0 - 100 °C
8.33 - 19.4 µin/in-°F

@Temperature 122 - 212 °F
longitudinal; ISO 11359-2
Raschig Group MELOPLAS® 152.7 MF
Cellulose-reinforced MF molding compound in white and colored shades. High surface hardness, very good UV stability, very good resistance to chemicals also to foodstuff ingredients, physiologically..
CTE, linear 15.0 - 35.0 µm/m-°C

@Temperature 50.0 - 100 °C
8.33 - 19.4 µin/in-°F

@Temperature 122 - 212 °F
ISO 11359-2
Raschig Group MELOPLAS® 181 MF
Cellulose-reinforced, phenol-modified MF molding compound (MPF) in white and colored shades. High surface hardness, good electrical properties, good mechanical strength, high UV and heat resistanc..
CTE, linear 15.0 - 35.0 µm/m-°C

@Temperature 50.0 - 100 °C
8.33 - 19.4 µin/in-°F

@Temperature 122 - 212 °F
ISO 11359-2
Raschig Group MELOPLAS® 181.5 MF
Cellulose-reinforced, phenol-modified MF molding compound (MPF) in white and colored shades. Very good electrical properties, high surface hardness, good mechanical strength, high UV and heat resis..
CTE, linear 15.0 - 35.0 µm/m-°C

@Temperature 50.0 - 100 °C
8.33 - 19.4 µin/in-°F

@Temperature 122 - 212 °F
ISO 11359-2
Raschig Group MELOPLAS® 182 MF
Wood flour-reinforced and inorganically filled, phenol-modified MF molding compound (MPF) in dark colors. Improved dimensional stability and electrical properties as compared with MP 180, high surf..
CTE, linear 15.0 - 35.0 µm/m-°C

@Temperature 50.0 - 100 °C
8.33 - 19.4 µin/in-°F

@Temperature 122 - 212 °F
ISO 11359-2
Raschig Group MELOPLAS® 183 MF
Cellulose-reinforced and inorganically filled, phenol-modified MF molding compound (MPF) in white and colored shades. Improved dimensional stability and electrical properties as compared with MP 18..
CTE, linear 15.0 - 35.0 µm/m-°C

@Temperature 50.0 - 100 °C
8.33 - 19.4 µin/in-°F

@Temperature 122 - 212 °F
ISO 11359-2
Raschig Group MELOPLAS® 2500 MF
Cellulose-reinforced MF molding compound in white and colored shades. Very good electrical properties, high surface hardness, good abrasion- and UV-stability, very good resistance to chemicals - al..
CTE, linear 15.0 - 35.0 µm/m-°C

@Temperature 50.0 - 100 °C
8.33 - 19.4 µin/in-°F

@Temperature 122 - 212 °F
ISO 11359-2
Raschig Group MELOPLAS® 3025 MF
Cellulose-reinforced and inorganically filled MF molding compound in white and colored shades. High surface hardness, good UV and heat stability, very good resistance to chemicals - also to foodstu..
CTE, linear 25.0 - 35.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
13.9 - 19.4 µin/in-°F

@Temperature -22.0 - 86.0 °F
TMA
SABIC Innovative Plastics NORYL HFM3015P PPE+PS (Asia Pacific)
30% GF/MF filled FR PPE/PS blend
CTE, linear 25.0 - 35.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
13.9 - 19.4 µin/in-°F

@Temperature -22.0 - 86.0 °F
TMA
SABIC Innovative Plastics NORYL CN1134 PPE+PS (Asia Pacific)
20% filled FR high modulus PPE/PS blend
CTE, linear 30.0 - 35.0 µm/m-°C
16.7 - 19.4 µin/in-°F
Master Bond Supreme 11AO Electrically Isolating Adhesive and Sealant
Description: Master Bond Polymer System SURPEME 11AO is a two component epoxy resin system for high performance bonding and sealing formulated to cure at room temperature or more rapidly at elevated..
CTE, linear 30.0 - 35.0 µm/m-°C

@Temperature 20.0 °C
16.7 - 19.4 µin/in-°F

@Temperature 68.0 °F
Abatron AboCast/AboCure 8109-2
High melting point. Filled version.Processing: 100/10 pbw; 90 minute potlife; mix at 130-140°C (270 °F); cures in 16 h/120°C (250°F), 10 h/140°C (285°F), 8 h/160°C (320°F), 2 h/ 200°C (390°..
CTE, linear 15.0 - 35.0 µm/m-°C

@Temperature 50.0 - 100 °C
8.33 - 19.4 µin/in-°F

@Temperature 122 - 212 °F
ISO 11359-2
Raschig Group MELOPLAS® 180 MF
Wood flour-reinforced, phenol-modified MF molding compound (MPF) in dark colors. High surface hardness, good mechanical strength and electrical properties, good heat resistance. Self-extinguishing ..
CTE, linear 24.0 - 35.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
13.3 - 19.4 µin/in-°F

@Temperature -22.0 - 86.0 °F
TMA
SABIC Innovative Plastics NORYL FM3020V PPE+PS (Asia Pacific)
30% filled FR high modulus foam grade
Copyright © lookpolymers.com All Rights Reserved