Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics NORYL HFM3015P PPE+PS (Asia Pacific)

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polystyrene (PS)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Noryl
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics NORYL HFM3015P PPE+PS (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
30% GF/MF filled FR PPE/PS blend
Physical Properties Metric English Comments
Specific Gravity 1.32 g/cc
1.32 g/cc
ASTM D792
Water Absorption 0.060 %

@Time 86400 sec
0.060 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0025 - 0.0030 cm/cm

@Thickness 3.20 mm
0.0025 - 0.0030 in/in

@Thickness 0.126 in
SABIC Method
Melt Flow 48.3 g/10 min

@Load 5.00 kg,
Temperature 300 °C
48.3 g/10 min

@Load 11.0 lb,
Temperature 572 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 98.0 MPa
14200 psi
SABIC - Japan Method
Elongation at Break 4.0 - 6.0 %
4.0 - 6.0 %
SABIC - Japan Method
Flexural Strength 137 MPa
19900 psi
ASTM D790
Flexural Modulus 7.64 GPa
1110 ksi
ASTM D790
Izod Impact, Notched 0.580 J/cm
1.09 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 25.0 - 35.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
13.9 - 19.4 µin/in-°F

@Temperature -22.0 - 86.0 °F
TMA
Deflection Temperature at 1.8 MPa (264 psi) 110 °C

@Thickness 6.40 mm
230 °F

@Thickness 0.252 in
unannealed; ASTM D648