Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 128 µm/m-°C | 71.0 µin/in-°F | ASTM E831 |
Quadrant EPP Acetron® MD Metal-detectable Copolymer Acetal (ASTM Product Data Sheet) Low moisture absorption High strength, stiffness Easy to machine No centerline porosity in Acetron® GP Many formulation options: Copolymer, Homopolymer, PTFE filled, and Internally lubricated/enha.. |
|||
CTE, linear | 128 µm/m-°C | 71.0 µin/in-°F | |
Saint-Gobain Rulon® AMR Bearing/Seal PTFE Same base material as Rulon AR but Rulon AMR contains a percentage of molybdenum disulfide for increased wear resistance and lower coefficient of friction. Typically used as a seal or gasket, Rulon .. |
|||
CTE, linear | 128 µm/m-°C | 71.1 µin/in-°F | Above Tg |
Epoxy Technology EPO-TEK® M10-D Epoxy Paste Material Description: A single component, B-stageable epoxy paste for semiconductor, microelectronics, and optical assemblies. It can be used in hybrid assemblies for lid-sealing and substrate atta.. |
|||
CTE, linear | 128 µm/m-°C | 71.1 µin/in-°F | Above Tg |
Epoxy Technology EPO-TEK® MA-5 Optical Grade Epoxy Material Description: A single component, B-stageable, optical grade epoxy for fiber optic assembly. It may be used for B-stage sealing of fiber cables into ferrules, or fiber optic feed through in.. |
|||
CTE, linear | 128 µm/m-°C | 71.1 µin/in-°F | Above Tg |
Epoxy Technology EPO-TEK® OE138 Two Component Epoxy Material Description: A two component epoxy with intermediate viscosity range between EPO-TEK® 353ND and EPO-TEK® 353ND-T. It is designed for semiconductor glob top applications, as well as use in.. |
|||
CTE, linear | 128 µm/m-°C | 71.0 µin/in-°F | ASTM D696 |
Ensinger TECAFLON™ PVDF Polyvinylidene Fluoride (PVDF) - extruded products Polyvinylidene fluoride, or PVDF, is a fluorinated thermoplastic resin which has good resistance to most mineral and organic acids, aliphatic and aromatic hydrocarbons, alcohols, halogenated solvent.. |
|||
CTE, linear | 128 µm/m-°C | 71.1 µin/in-°F | Silicone Property; ASTM E 831 |
Arlon Thermabond® 99A60X008 0.008" (0.203 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Description: Primerless Thermabond®: Electrically insulating, thermally conductive, electronic adhesive. Bonds without primer.Design/Construction: Liner: FEPProduct: Uncured Silicone Rubber Carrier.. |
|||
CTE, linear | 128 µm/m-°C | 71.1 µin/in-°F | Silicone Property; ASTM E831 |
Arlon Thermabond® R37300X008 0.008" Uncured Silicone Rubber on Fiberglass Carrier Primerless Thermabond®: Electrically insulating, thermally conductive, electronic adhesive. Bonds without primer.Design/Construction:Liner: 1 mil FEPProduct: Uncured Silicone RubberCarrier: 3 m.. |
|||
CTE, linear | 128 µm/m-°C @Temperature 20.0 °C |
71.1 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Ensinger ENSIKEM® PVDF (Polyvinylidene Fluoride) - Extruded Products
(discontinued **) Polyvinylidene fluoride, or PVDF, is a fluorinated thermoplastic resin that has outstanding resistance to most mineral and organic acids, aliphatic and aromatic hydrocarbons, alcohols, halogenated s.. |