Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 128 µm/m-°C | 71.0 µin/in-°F | ASTM E831 |
Quadrant EPP Acetron® MD Metal-detectable Copolymer Acetal (ASTM Product Data Sheet) Low moisture absorption High strength, stiffness Easy to machine No centerline porosity in Acetron® GP Many formulation options: Copolymer, Homopolymer, PTFE filled, and Internally lubricated/enha.. |
|||
CTE, linear | 128 µm/m-°C | 71.0 µin/in-°F | |
Saint-Gobain Rulon® AMR Bearing/Seal PTFE Same base material as Rulon AR but Rulon AMR contains a percentage of molybdenum disulfide for increased wear resistance and lower coefficient of friction. Typically used as a seal or gasket, Rulon .. |
|||
CTE, linear | 128 µm/m-°C | 71.0 µin/in-°F | ASTM D696 |
Ensinger TECAFLON™ PVDF Polyvinylidene Fluoride (PVDF) - extruded products Polyvinylidene fluoride, or PVDF, is a fluorinated thermoplastic resin which has good resistance to most mineral and organic acids, aliphatic and aromatic hydrocarbons, alcohols, halogenated solvent.. |