Saint-Gobain Rulon® AMR Bearing/Seal PTFE

Category Polymer , Thermoplastic
Manufacturer Saint-Gobain Perfomance Plastics
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Saint-Gobain Rulon® AMR Bearing/Seal PTFE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Same base material as Rulon AR but Rulon AMR contains a percentage of molybdenum disulfide for increased wear resistance and lower coefficient of friction. Typically used as a seal or gasket, Rulon AMR is specified in many military and commercial applications for hydraulic and pneumatic controls.Information provided by distributor TriStar Plastics Corp.
Physical Properties Metric English Comments
Density 2.30 g/cc
0.0831 lb/in³
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
Tensile Strength, Yield 10.3 MPa
1500 psi
Elongation at Break 130 %
130 %
Flexural Strength 4.14 MPa
600 psi
Izod Impact, Notched 3.20 J/cm
6.00 ft-lb/in
Coefficient of Friction, Dynamic 0.010
0.010
Dry vs. Steel
Coefficient of Friction, Static 0.025
0.025
Dry vs. Steel
Limiting Pressure Velocity 0.350 MPa-m/sec
10000 psi-ft/min
Thermal Properties Metric English Comments
CTE, linear 128 µm/m-°C
71.0 µin/in-°F
Thermal Conductivity 0.331 W/m-K
2.30 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 288 °C
550 °F
Continuous
316 °C
600 °F
Short Term
Deflection Temperature at 1.8 MPa (264 psi) 116 °C
240 °F
Minimum Service Temperature, Air -240 °C
-400 °F
Embrittlement Temp
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
Dielectric Constant 2.5

@Frequency 1.00e+6 Hz
2.5

@Frequency 1.00e+6 Hz
Dielectric Strength 14.8 kV/mm
375 kV/in
Short Term